Demarcating the Effects of Aliphatic Ester Chain Lengths and Molecular Weight on Electrode-Electrolyte Interphase Formation for Wide-Temperature Operation of Lithium-Ion Batteries.
Thomas J Watts, Marshall C Smart, Arumugam Manthiram
Walker Department of Mechanical Engineering, The University of Texas at Austin, Austin, Texas78712, United States. · Jet Propulsion Laboratory, California Institute of Technology, 4800 Oak Grove Drive, Pasadena, California91109, United States.
Key points
From the paper's conclusion- This study investigates the molecular origin of aliphatic ester alkyl and alkoxy chain length effects on electrolyte solvation, decomposition, and electrochemical performance of LIBs within a wide-temperature range of -60 to +60 °C using Li1.02Ni0.8Mn0.1Co0.1O2 (NMC811) cathode and graphite anode full cells.
- Removal of the alkyl chain and lengthening of the alkoxy chain improved low-temperature conductivity, enabling 110 mAh g-1 of C/10 discharge capacity at -60 °C, and 122 mAh g-1 of reversible capacity when cycling at -40 °C.
- This work establishes a structure-property framework grounded in the intrinsic electronic structure of the ester chain lengths for tuned ester-electrolyte design for wide-temperature LIB operation.
Abstract
Conventional nonaqueous electrolytes for lithium-ion batteries (LIBs) employ carbonate cosolvents to dissociate the Li+ salt. Aliphatic esters can be substituted to lower the melting point of the electrolyte solution, improving low-temperature performance, but suffer from deleterious surface film formation. This work identifies the molecular origin of aliphatic ester alkyl and alkoxy chain length effects on electrolyte solvation, decomposition, and electrochemical performance of LIBs within a wide-temperature range of -60 to +60 °C in Li1.02Ni0.8Mn0.1Co0.1O2 (NMC811) cathode and graphite anode full cells. Removal of the alkyl chain and lengthening of the alkoxy chain improves low-temperature conductivity at temperatures below -40 °C, enabling 110 mAh g-1 of C/10 discharge capacity at -60 °C, and 122 mAh g-1 of reversible capacity when cycling at -40 °C. Long alkoxy esters are shown to exhibit greater reactivity with both electrodes, and their decomposition products were identified by nuclear magnetic resonance (NMR) spectroscopy and X-ray photoelectron spectroscopy (XPS). Ternary solvent blends were then developed to limit the reactivity of the esters and improve the +60 °C cycling performance at the expense of the -60 °C discharge capacity. This work establishes a structure-property framework, grounded in the intrinsic electronic structure of the ester chain lengths, for tuned ester-electrolyte design for wide-temperature LIB operation.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- This study investigates the molecular origin of aliphatic ester alkyl and alkoxy chain length effects on electrolyte solvation, decomposition, and electrochemical performance of LIBs within a wide-temperature range of -60 to +60 °C using Li1.02Ni0.8Mn0.1Co0.1O2 (NMC811) cathode and graphite anode full cells.
- Removal of the alkyl chain and lengthening of the alkoxy chain improved low-temperature conductivity, enabling 110 mAh g-1 of C/10 discharge capacity at -60 °C, and 122 mAh g-1 of reversible capacity when cycling at -40 °C.
- This work establishes a structure-property framework grounded in the intrinsic electronic structure of the ester chain lengths for tuned ester-electrolyte design for wide-temperature LIB operation.
Readers' thoughts
No reader thoughts yet.
Related papers
- Steric-Electronic Engineering of Ester Carbonyls Enables Thermodynamic-Kinetic Regulation of Electron Transfer for High-Voltage and High-Rate Lithium Metal Batteries.Angewandte Chemie (International ed. in English) · 2026
- A Three-Descriptor Framework for Solvation Design of Low-Temperature Electrolytes in Lithium Batteries.Journal of the American Chemical Society · 2026
- Flame-retardant electrolytes with electrochemically-inert and weakly coordinating dichloroalkane diluents for practical lithium metal batteriesNature Communications · 2025
- Rational electrolyte solvent screening for high-energy lithium metal batteries at low temperaturesNature Communications · 2025
- Alkoxyethyl Acetate Electrolytes for High-Voltage Lithium Metal Batteries.Angewandte Chemie (International ed. in English) · 2026
- Role-Differentiated Solvation Directs Interfacial Chemistry in Wide-Temperature Lithium Metal Batteries.Angewandte Chemie (International ed. in English) · 2026