Local Coordination Motif Compatibility Induces the Formation of Shortened Fe3+-O-Ni3+δ Moieties as Active Sites for Highly Efficient Oxygen Evolution Reaction.
Wenchao Wan, Liqun Kang, Shiqian Wei, Alexander Schnegg, Kaltum Abdiaziz, Longxiang Liu, Fei Guo, Christopher S Allen,
Max Planck Institute for Chemical Energy Conversion , Stiftstraße 34-36, Mülheim an der Ruhr45470, Germany. · Leshan West Silicon Materials Photovoltaic New Energy Industry Technology Research Institute, Leshan614000, China.
Key points
From the paper's conclusion- DFT calculations reveal that the unusually short Fe3+-O bond leads to a moderate *O adsorption strength at the Fe site in the catalyst, thereby creating the most favorable conditions for the oxygen evolution reaction (OER).
Abstract
NiFe-based compounds are among the most promising catalysts for the oxygen evolution reaction (OER). However, the structural reconstruction of NiFe catalysts during OER is not fully understood. Most existing studies implicitly assume the formation of a homogeneous NiFe (oxy)hydroxide lattice; however, the actual reconstruction process is more likely to generate structurally heterogeneous (oxy)hydroxide phases with local distortions due to the intrinsic mismatch between Fe3+-O and Ni3+-O bond lengths in the bulk NiFe compounds. By constructing atomically dispersed Ni and Fe active sites as precatalysts and combining them with operando spectroelectrochemical studies, we observed an unusual reconstruction pathway in which isolated Ni2+ and Fe atoms can adaptively evolve into a short-range mixed NiFe (oxy)hydroxide local structure through the formation of interconnected M-O-M' (M/M' = Ni3+δ, Fe3+) motifs during the OER. At 1.6 V vs RHE, the reconstructed γ-Fe3+OOH clusters are induced to integrate into the high-valent γ-Ni3+δOOH lattice, resulting in a short-range mixed NixFe1-xOOH structure. This new structure is characterized by an unusually short Fe3+-Ni3+δ distance of ∼2.86 Å, which is significantly shorter than the typical Fe3+-Fe3+ distance in Fe3+ (oxy)hydroxides (2.95-3.25 Å). Interestingly, this "induction effect" is absent in Co3+-Fe3+ catalysts, as atomically dispersed Co3+ sites directly transition into γ-Co3+OOH, which lacks structural compatibility with γ-Fe3+OOH. DFT calculations reveal that the unusually short Fe3+-O bond leads to a moderate *O adsorption strength at the Fe site in the catalyst, thereby creating the most favorable conditions for the oxygen evolution reaction (OER).
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Synergistic microstructural optimization of nickel-iron dual sites in NiFealloy/NiFe2O4 by La doping and V vacancies for boosting the oxygen evolution reaction.Nanoscale · 2026
- Surface Reconstruction‐Promoted Alkaline Overall Water Splitting on Fe‐Doped Ni₂ P/NiMoO₄ Composite StructureElectron · 2026
- Lattice Oxygen–Mediated Water Oxidation on Reconstructed Ni₃ S₂ /NiFeOOH HeterointerfacesChemistry - A European Journal · 2025
- Guest-Matched Encapsulation in Ni-MOF-274 for Phase-Controlled FeNi Alloy Electrocatalysts toward Oxygen Evolution.Inorganic chemistry · 2026
- Fe incorporation pathway encodes spatial memory during metal-organic framework reconstruction for oxygen evolution.Journal of colloid and interface science · 2026
- Surface reconstruction of FeMnP@NiFe LDH core-shell heterostructure with interfacial electronic effect for oxygen evolution.Journal of colloid and interface science · 2026