Deprotonation-Induced Strong Covalent Interfacial Bonding Stabilizes the Solid Electrolyte Interphase and Raises the Performance of Lithium-Ion Batteries
Fei Wang, Zhendong Liu, Jingyuan Li, Shuqi Wang, Lewis Kien Juen Ting, Yulin Gao, Xingyang Wang, Baptiste Py,
National University of Singapore · Fujian Research Institute of Light Industry
Key points
From the paper's conclusion- The present work reveals the deprotonation-driven interphase stability mechanism and establishes active-component regulation as a new paradigm for high-energy density lithium-ion batteries.
Abstract
Chemically stable interfaces in electrodes are indispensable for maintaining the robust electrochemical interphase evolution to ensure long-term cycling stability of lithium-ion batteries. However, the potential impact on interfacial chemistry by residual protons in association with carboxyl and hydroxyl groups in water-soluble binders (e.g., PAA, CMC/SBR), which are inevitably introduced during the slurry-casting fabrication of electrodes, has received limited attention. Herein, we uncover that the chemically reactive protons trigger ethylene carbonate ring-opening reactions, thereby disrupting the solid electrolyte interphase (SEI) formation and stability, ultimately degrading battery performance. Building on this new insight, a chemically stable, deprotonated electrode (DE) featuring much reinforced interfaces arising from heterogeneous carbon–oxygen covalent bonds is developed, which enables stronger chemical anchoring than the hydrogen bond interactions by carboxyl and hydroxyl groups. In addition, the thus-developed oxygen-rich deprotonated interface reshapes the formation of an inner Li 2 O-dominated SEI. This deprotonation approach demonstrates broad compatibility with several anode active materials, including microsized SiO, Si, graphite, and their composites. For example, DEs with 86 wt·% SiO/graphite and 80 wt·% 5 μm-sized Si deliver 5.14 mAh·cm –2 over 500 cycles and 4.32 mAh·cm –2 over 200 cycles, respectively. With the new DEs, two Ah-level cells paired with LiNi 0.6 Co 0.2 Mn 0.2 O 2 and LiNi 0.8 Co 0.1 Mn 0.2 cathodes achieve the respective gravimetric energy densities of 288 Wh·kg –1 and 424 Wh·kg –1, while maintaining the capacity retention of 81% over 300 and 78% over 600 cycles. The present work reveals the deprotonation-driven interphase stability mechanism and establishes active-component regulation as a new paradigm for high-energy density lithium-ion batteries.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- A Balance-of-Charges Descriptor for Electron-Delocalized Solvents Enables Calendar-Stable and Thermally Tolerant Silicon-Based Anodes.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Coulomb trapping of ions in a solid electrolyte interphase by deprotonation-induced surface charges.Physical chemistry chemical physics : PCCP · 2026
- Lithiated PAA‐Coated SiOₓ Anode for Stable and High‐Capacity Lithium‐Ion Batteries: Interfacial Regulation and Volume Expansion SuppressionSmall · 2026
- Proton-Mediated Dynamic Interfacial Regulation in a Covalent Polymer Anode for Stable Aqueous Calcium-Ion Batteries.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Pre‐Constructed Mechano‐Electrochemical Adaptive Solid Electrolyte Interphase to Enhance Li⁺ Diffusion Kinetics and Interface Stability for Chemically Prelithiated SiO AnodesAdvanced Science · 2025
- Dynamic Interfacial S-O Bonding Stabilizes Oxygen Redox Through Reversible Electron Confinement.Advanced materials (Deerfield Beach, Fla.) · 2026