Integrated Solvation Chemistry Enables High Energy Li Metal Batteries
Yuntong Ma, Haikuo Zhang, Shihao Duan, Baochen Ma, Shuo‐Qing Zhang, Ling Lv, Long Chen, Tao Zhou,
Hangzhou Wanxiang Polytechnic · ASM International (Finland)
Key points
From the paper's conclusion- Here, we propose a solvation integration strategy that confines both solvent molecules and anions within the first solvation sheath, thereby minimizing their reactivity.
Abstract
Rational electrolyte design for high-energy Li metal batteries (LMBs) demands the simultaneous suppression of solvent reactivity and the promotion of anion reduction. However, existing approaches often fall short due to inadequate control over the solvation structure, leading to excessive free solvent and anion species and continual side reactions. Here, we propose a solvation integration strategy that confines both solvent molecules and anions within the first solvation sheath, thereby minimizing their reactivity. As a proof of concept, we employ lithiophilic (trifluoromethoxy)fluorobenzene (TFMFB) to tune Li + solvation by enhancing the affinity of solvents toward Li +, ensuring favorable Li + kinetics. Simultaneously, lipophilic (trifluoromethyl)cyclohexane (FMCH) forms an outer-layer kinetic barrier that inhibits solvent/anion desolvation. This inner-lithiophilic and outer-lipophilic configuration creates synergistic confinement, significantly enhancing oxidation stability and enabling robust interfacial chemistry. As a result, an anode-free Cu∥LiNi 0.5 Co 0.2 Mn 0.3 O 2 (NCM523) pouch cell utilizing the tailored solvation-integrated electrolyte (SIE) achieves 80% capacity retention after 120 cycles. Furthermore, the aggressive 10 Ah Li∥LiNi 0.9 Co 0.05 Mn 0.05 O 2 (NCM955) pouch cell with an ultralean electrolyte (1.1 g Ah –1 ) delivers an ultrahigh energy density of 568 Wh kg –1 . This solvation integration concept provides a promising guideline for the electrolyte design toward practical high-energy LMBs.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Core–Shell Solvation Structure Engineering Enables Practical Lithium Metal Batteries With 475 Wh Kg −1Advanced Functional Materials · 2026
- Engineering Anion-Solvent Interactions to Modulate Ion Pairing and Accelerate Desolvation in High-Voltage Lithium-Metal Batteries.ACS nano · 2026
- Solvation Cluster Engineering of Non-Fluorinated Ethers toward High-Energy Lithium Metal Batteries.Journal of the American Chemical Society · 2026
- Additive strongly-coordinated solvation structure towards high-voltage 600 Wh/kg-class lithium metal pouch cell.Nature communications · 2026
- Anionic solvation reconstruction stabilizes interfacial chemistry for high-temperature and high-voltage Li metal batteries.Nature communications · 2026
- Role-Differentiated Solvation Directs Interfacial Chemistry in Wide-Temperature Lithium Metal Batteries.Angewandte Chemie (International ed. in English) · 2026