Nanoscale Core–Shell Catalysts for H₂ Production by Methane Decomposition: Supported Nickel Nanoparticles Ensheathed in Metal Oxides
Qiangqiang Xue, Shuairen Qian, Kang Hui Lim, Melvin Xin Jie Wee, Kaiqi Nie, Shuwen Cheng, Xiaohan Chen, Prae Chirawatkul,
National University of Singapore · State Key Laboratory of Chemical Engineering
Key points
From the paper's conclusion- We now report the design and synthesis of supported Ni catalysts that address these limitations; they consist of silica-supported Ni nanoparticles ensheathed in nanoscale TiO 2 shells, forming an embedded core–shell structure that provides catalyst stability, maintaining a H 2 site-time yield of 3.6 mol/g Ni /h at a space velocity of 24000 mL g cat –1 ·h –1 at 550 °C for 6 h on stream in a flow re
Abstract
Catalytic methane decomposition provides a potentially viable route to low-cost, CO x -free H 2 from this abundant source. A remaining challenge is to facilitate the needed low-temperature C–H bond activation with high catalytic activity and stability. We now report the design and synthesis of supported Ni catalysts that address these limitations; they consist of silica-supported Ni nanoparticles ensheathed in nanoscale TiO 2 shells, forming an embedded core–shell structure that provides catalyst stability, maintaining a H 2 site-time yield of 3.6 mol/g Ni /h at a space velocity of 24000 mL g cat –1 ·h –1 at 550 °C for 6 h on stream in a flow reactor. In contrast, a comparable catalyst without the sheath deactivated after only 2.5 h, being characterized by a Ni-extracting tip-growth mechanism of coproduct carbon nanotube formation that destroyed the catalyst. An advantage of the ensheathed catalyst is that it facilitates a Ni-sparing base-growth mechanism. Infrared and Raman spectra, combined with other catalyst characterization data and calculations at the level of density functional theory, show that the TiO 2 sheaths barely hinder the C–H bond cleavage and carbon nanotube formation on the underlying nickel, while providing the advantages stated above. We postulate that these results provide guidance for the synthesis of catalysts for low-temperature H 2 production and related reactions requiring C–H bond activation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Robust α-NiMoO₄ /MoS₂ Catalysts for Low-Temperature Methane Pyrolysis: Synergistic Ni–Mo–S Interactions for Sustainable Hydrogen Production with Selective Carbon Nanotubes/GrapheneACS Sustainable Chemistry & Engineering · 2025
- Dual Active Sites of Ni‐O‐Ti on NiTiO₃ Coated Ni for Efficient and Robust Photothermal CO₂ MethanationAdvanced Energy Materials · 2026
- Cu0/Cu+ Interfacial Sites on Activated Carbon for Regenerable CO2–Free Hydrogen Production via Methane DecompositionIndustrial & Engineering Chemistry Research · 2026
- Iron-Based Catalysts on Tailored Alumina Supports for COx-Free Methane Decomposition to H2 and Carbon.ChemistryOpen · 2026
- Reaction-driven adaptive restructuring of a Ni/SiO2 catalyst enables long-term stability in dry reforming of methane.Nanoscale · 2026