ACS Sustainable Resource Management

Recovery of Rare-Earth Elements from Bauxite Residue Using Carbonate Lixiviants and Gas Carbonation

Alexander V. Boyarintsev, Sergei I. Stepanov, Htet Ye Aung, Pavel I. Ivanov, Ekaterina V. Boyarintseva, Galina V. Kostikova, Valeriy I. Zhilov, Aslan Yu. Tsivadze

Key points

From the paper's conclusion
  • The possibility of accumulating Sc, Y, and Ln in carbonate solutions to obtain rough concentrates containing up to 5–14% Sc2O3, and 7–9% total REE oxides was also confirmed.

Abstract

The production of rare-earth elements (REEs) has become a crucial component of modern technological development, requiring an expanded raw material base. The raw material aspect of the REE problem involves searching for the most cost-effective and stable byproduct sources of REEs. Alumina production waste, namely, bauxite residue (BR) or red mud, could become such a source in the near future through comprehensive processing. Alternative nonacid (carbonate–alkaline) preferential hydrometallurgical approaches are promising for establishing energy- and resource-saving, economically viable, comprehensive BR processing. This article presents quantitative data on the distribution of Sc, Y, and Ln into the liquid phase for the heterogeneous systems “stockpiled BR” − M2CO3−CO2−H2O (where M = Na+ or NH4+), both in the absence and presence of complexing agents (Na2H2EDTA and HOx), NaCl, and mechanical intensification. The possibility of organizing multiple recycling of carbonate solutions, as well as utilizing CO2 gas as a reagent for neutralizing alkali and for pH control, was confirmed. The principal factors increasing REE recovery during BR leaching in carbonate media have been determined. It is demonstrated that mechanical (ultrasonication) and chemical (complexing ligand supplementation) intensification under gas carbonation conditions decreases the leaching duration and increases the recovery of valuable microcomponents. Approaches are proposed to prevent the hydrolytic precipitation of Sc and REEs, thereby achieving a single-step leaching yield of over 40–45% for Sc and up to 60–65% for medium-heavy REEs. The possibility of accumulating Sc, Y, and Ln in carbonate solutions to obtain rough concentrates containing up to 5–14% Sc2O3, and 7–9% total REE oxides was also confirmed. Laboratory tests demonstrated the feasibility of recovering Y and Ln as byproducts along with Sc from BR using a direct carbonation leaching process. This enables the development of environmentally safe and resource-saving methods for the comprehensive treatment of alkaline alumina production waste, providing a viable pathway for manufacturing commercial products.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers