ACS Sustainable Chemistry & Engineering

Sacrificial-Anion Reinforced Weak-Solvation Electrolyte Enables High-Voltage-Tolerant Sodium-Ion Batteries at –40 °C

Lin Wang, Long Wang, Jing Zhou, Yu Cao

Key points

From the paper's conclusion
  • Consequently, the Na3V2(PO4)3 (NVP)||Na half cell retains a reversible capacity of 71.6 mAh g–1 after 170 cycles at –40 °C and 4.3 V, while the NVP||hard carbon full cell delivers 60 mAh g–1 at –40 °C with 91% capacity retention after 120 cycles at 1 C.

Abstract

Sodium-ion batteries (SIBs) are promising candidates for large-scale energy storage due to abundant and low-cost sodium resources. However, their practical operation is severely hindered by sluggish Na+ transport kinetics at sub-zero temperatures and unstable electrode/electrolyte interfaces under high-voltage conditions. Herein, we develop a sacrificial-anion reinforced weak-solvation (SAR-WS) electrolyte for high-voltage-tolerant and low-temperature SIBs. The low-viscosity, weakly solvating THF-based solvent facilitates rapid bulk Na+ migration and reduces desolvation resistance, while ClO4– introduced by the low-content NaClO4 additive participates in the primary Na+ solvation sheath and preferentially decomposes at the cathode interface, inducing the formation of a multicomponent inorganic-rich CEI that suppresses solvent oxidation and stabilizes the cathode interface. Consequently, the Na3V2(PO4)3 (NVP)||Na half cell retains a reversible capacity of 71.6 mAh g–1 after 170 cycles at –40 °C and 4.3 V, while the NVP||hard carbon full cell delivers 60 mAh g–1 at –40 °C with 91% capacity retention after 120 cycles at 1 C. This work presents a sacrificial sodium-salt additive strategy to reconcile weak-solvation-enabled low-temperature kinetics with anion-derived high-voltage interfacial stability in SIB electrolytes.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers