From the paper's conclusion- Overall, the Sb2S3 (35 min)/ZnO heterostructure provided the best compromise, combining the highest crystalline quality and the lowest effective band gap with a photocurrent only slightly lower than that of the 30 min sample, highlighting its potential for low-cost thin-film photovoltaic devices.
Abstract
Sb2S3/ZnO heterostructures were fabricated by chemical bath deposition (CBD) of Sb2S3 for 30, 35, and 40 min, yielding thicknesses of 252, 311, and 387 nm, followed by vacuum annealing at 350 °C and atomic layer deposition (ALD) of a 44 nm ZnO layer at 200 °C. The influence of the absorber deposition time on the structural, morphological, optical, and photoelectrical properties was evaluated. X-ray diffraction confirmed orthorhombic Sb2S3, hexagonal ZnO, and a secondary Sb2O3 phase whose fraction increased from 9.0% (30 min) to 14.7% (40 min). Rietveld refinement showed that the Sb2S3 fraction increased from 28.5% (30 min) to 43.4% (35 min) and remained constant at 40 min, while the ZnO fraction decreased from 62.5% to 41.9%. Williamson–Hall analysis yielded crystallite sizes of 29.1, 36, and 20.1 nm and dislocation densities of 1.17, 0.77, and 2.46 × 10–3 nm–2 for the 30, 35, and 40 min samples, respectively. SEM revealed wheat-like grains at 30 and 40 min and rosette-like clusters with coarser, elongated grains at 35 min. The 35 min sample also exhibited the highest Zn and lowest O contents by EDS. The effective band gaps were 2.3, 1.6, and 2.1 eV, respectively, governed by the Sb2S3 fraction, crystalline quality, and oxide content. All heterostructures exhibited a photoresponse that decreased with increasing absorber thickness, with the 30 min sample showing the highest photocurrent. Overall, the Sb2S3 (35 min)/ZnO heterostructure provided the best compromise, combining the highest crystalline quality and the lowest effective band gap with a photocurrent only slightly lower than that of the 30 min sample, highlighting its potential for low-cost thin-film photovoltaic devices.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Design and numerical analysis of antimony trisulfide (Sb 2 S 3 ) solar cell using SCAPS-1D softwareEngineering Research Express · 2026
- Antimony Oxide Enabled Ion‐Dominant Deposition for High‐Efficiency Sb₂ S₃ Solar CellsAdvanced Functional Materials · 2026
- Conformal PAA-Modified SnO2 Interfacial Layer for Efficient and Stable Sb2S3 Solar Cells.Langmuir : the ACS journal of surfaces and colloids · 2026
- Mitigating the Optical-Electrical Trade-Off in Sb2S3 Solar Cells with a Buried Li-Modified ZnO InterlayerACS Energy Letters · 2026
- Enhancing Sb2S3 thin film quality through controlled sulfurization: A study on temperature and pressure variationsResults in Engineering · 2026
- Atomic-Layer-Deposited Interlayers Enabling Interfacial Band Tuning in Vapor Transport Deposition-SnS/CdS Solar CellsACS Applied Energy Materials · 2026