PEG Middle-Block Molecular Weight as a Quantitative Design Variable for Stereocomplex Formation Efficiency in High-Molecular-Weight PLLA-PEG-PLLA/PDLA Blends.
Dutchanee Pholharn, Samaneh Dehghani, Onpreeya Veang-In, Yottha Srithep
Department of Chemistry, Faculty of Science and Technology, Rajabhat Mahasarakham University, Mahasarakham 44000, Thailand. · Department of Wind Energy, Kunsan National University, Gunsan 54150, Republic of Korea.
Key points
From the paper's conclusion- Here, we demonstrate that the PEG middle-block molecular weight in PLLA-PEG-PLLA triblock copolymers is the decisive kinetic control variable governing SC formation efficiency (f SC).
Abstract
Achieving complete stereocomplex (SC) formation in high-molecular-weight PLLA/PDLA blends by injection molding remains a challenge because the rapid mold-cooling rate suppresses the slow enantiomeric chain-recognition process. Here, we demonstrate that the PEG middle-block molecular weight in PLLA-PEG-PLLA triblock copolymers is the decisive kinetic control variable governing SC formation efficiency (f SC). Copolymers with PEG M n = 400, 4000, and 35,000 g/mol were synthesized by bulk ring-opening polymerization (ROP) at two PLLA-block M n targets (100,000 and 200,000 g/mol) and blended 1:1 with PDLA before injection molding. W PLA-corrected differential scanning calorimetry (DSC) showed that f SC increased monotonically from approximately 75-76% (PEG400) to 93-95% (PEG4k) and to 100% (PEG35k), where the value was confirmed independently by X-ray diffraction (XRD). PEG35k-containing SC specimens crystallized completely during mold cooling without any postcooling cold crystallization, establishing M n,PEG ≥ 35,000 g/mol as the practical threshold for complete in-mold stereocomplex at M n ≈ 200,000 g/mol without postprocessing annealing. Toughness increased 7.1-fold, from 10.1 MJ m-3 (neat PLLA) to 71.5 MJ m-3 (L100 K-35k-L100 K/PDLA), driven by synergistic PEG-induced ductility and SC crystal reinforcement. All SC-PLLA-PEG-PLLA specimens maintained dimensional stability at 200 °C, whereas non-SC counterparts melted.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Preparation of green high-performance PLA stereocomplexes and rigid-flexible segment competition.Soft matter · 2026
- The Effect of Molecular Chain Entanglement Regulated by Different Shear Conditions on Stereocomplex Crystallization in the PLLA/PDLA BlendIndustrial & Engineering Chemistry Research · 2026
- Non-equimolar stereocomplex polylactide fibers strengthen and toughen poly(L-lactic acid) via interfacial stereocomplexation while retaining transparency.International journal of biological macromolecules · 2026
- Stereocomplex crystallite-mediated modification of poly(lactic acid)-based composites.International journal of biological macromolecules · 2026
- Tailoring the Morphology and Properties of Stereocomplex‐Type Porous Poly(Lactic Acid) Materials via Poly(ε‐Caprolactone) IncorporationPolymer Engineering & Science · 2026
- Solvent Evaporation-Controlled Stereocomplexation in PLLA/PDLA Films for Sustainable PackagingPolymers · 2026