Degradation Behavior of NBR Seals Exposed to Halogenated Olefins under Coupled Thermal and Mechanical Loads: A Multiscale Experimental and Computational Study.
Junjie Fang, Yujia Huo, Jin Wang, Xin Huang, Xiaomeng Zhou
Key Laboratory of Civil Aviation Thermal Hazards Prevention and Emergency Response, Civil Aviation University of China, Tianjin 300300, P. R. China.
Key points
From the paper's conclusion- These findings elucidate the degradation mechanisms of NBR seals and provide practical engineering guidance for material selection and failure prevention, contributing to safer process design with halogenated olefins.
Abstract
Halogenated olefins are promising low-GWP substitutes for traditional halocarbons in refrigeration, fire protection, and energy storage, but their compatibility with elastomeric seals poses a potential safety risk in process systems. This study systematically investigates the degradation behavior of nitrile butadiene rubber (NBR) exposed to five representative halogenated olefins-namely, 2-bromo-3,3,3-trifluoropropene (2-BTP), 2-chloro-3,3,3-trifluoropropene (R1233xf), 2,3,3,3-tetrafluoropropene (R1234yf), cis-1,3,3,3-tetrafluoropropene (R1234ze-(Z)), and trans-1,3,3,3-tetrafluoropropene (R1234ze-(E))-under simulated service conditions (0-70 °C, 0-2000 N compressive load, 15-45 days). Overall, the performance evolution of NBR exhibits a strong dependence on environmental conditions, and is closely correlated with the molecular architecture of halogenated olefins. 2-BTP caused the most severe damage (compression set: 31.18%; hardness loss: 14.38%; compressive strength loss: 41.35%), while fluorinated olefins showed weaker effects. Microscopic and spectroscopic analyses confirmed surface roughening, microcracking, halogen penetration, and formation of C-X (X = F, Cl, Br) bonds. Molecular dynamics simulations revealed that thermal energy weakens intermolecular interactions, whereas compressive stress induces chain orientation and free-volume redistribution, synergistically enhancing diffusion. The diffusion coefficients follow R1234ze-(E) > R1234yf > R1234ze-(Z) > R1233xf >2-BTP. Density functional theory calculations confirm that halogen radicals attack NBR's CC and -CN groups via low-barrier pathways. These findings elucidate the degradation mechanisms of NBR seals and provide practical engineering guidance for material selection and failure prevention, contributing to safer process design with halogenated olefins.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mechanical Properties Evolution and Aging Mechanism of NBR Sealing Materials Under Multiple Environmental Factors in Ultra-High Voltage Converter Station.Polymers · 2026
- Hydrogen Transport, Viscoelastic Drift, and Multiscale Characterization Framework for Elastomeric Seals Under High-Pressure HydrogenPolymers · 2026
- Reliability study of fluorosilicone rubber for liquid impregnated capacitors in cold regionsJournal of Physics: Conference Series · 2026
- Development and Performance of Elastomer Seals for Hydrogen Storage and Distribution Systems: Challenges, Solutions, and Future Perspectives. Part I: The Influence of Pressurized Hydrogen on Materials for Elastomer SealsHydrogen · 2026
- Polymeric Sealing Materials in Pneumatic Actuators: From Degradation Mechanisms to Failure Diagnostics and Service-Life Prediction.Materials (Basel, Switzerland) · 2026
- Impacts of extreme low-temperature on the properties of the benzyl toluene-impregnated gasket silicone rubber for capacitor applicationJournal of Physics: Conference Series · 2026