Structure-Processing-Property Relationships in PVOH/PBAT Blends Plasticized with Dipentaerythritol, ε‑Caprolactone, and Water.
Sakib Khan, Abu Saifullah, Zhongyi Zhang, Hom N Dhakal
School of Electrical and Mechanical Engineering, University of Portsmouth, Portsmouth PO1 3DJ, U.K.
Key points
From the paper's conclusion- These findings position ternary hydrogen-bond engineering as a reaction-free, melt-processing route to property-tunable PBAT/PVOH films for biodegradable flexible packaging.
Abstract
Water-soluble poly-(vinyl alcohol) (PVOH) offers high tensile strength and an excellent oxygen barrier, but its dense hydrogen-bond network places its melting point close to its decomposition temperature, making it difficult to melt-process. Poly-(butylene adipate-co-terephthalate) (PBAT) is melt-processable and ductile but has low strength and dimensional stability that restrict its use. To combine their strengths, PBAT/PVOH blends (10-40 wt % PBAT) were melt-compounded with a 20 wt % ternary plasticizer of dipentaerythritol, ε-caprolactone, and water in equal parts, benchmarked against a water-only control at 40 wt % PBAT. Across FTIR, XRD, DSC, steady-shear and oscillatory rheology, DMA, tensile, SEM, AFM, TGA, and gas-barrier measurements, the ternary plasticizer governs the structure-property relationship by redistributing the PVOH hydrogen-bond network rather than breaking it; it broadens and shifts the O-H stretching envelope, suppresses PVOH crystallinity and recrystallization, depresses the glass transition by 17-27 °C, and broadens the relaxation spectrum, with no cross-linking or covalent grafting. Composition sets the phase topologydispersed PBAT domains at 20-30 wt % and a cocontinuous structure at 40 wt %while the plasticizer controls interfacial adhesion, converting the weakly bonded, void-laden interfaces of the water-only control into well-adhered ones. Among the series, the 20 wt % blend (PBAT-20) gives the best stiffness-toughness balance (modulus ≈ 0.23 GPa, ultimate tensile strength ≈ 20 MPa) together with an oxygen transmission rate of ≈6.4 cm3 m-2 day-1 for a 400 μm film, equivalent to ≈102 cm3 m-2 day-1 when normalized to a 25 μm thickness. The water-vapor transmission rate of the same film remains high (6.06 g m-2 day-1), so the films reported here are suited to oxygen-sensitive but moisture-tolerant applications rather than to moisture-critical ones. These findings position ternary hydrogen-bond engineering as a reaction-free, melt-processing route to property-tunable PBAT/PVOH films for biodegradable flexible packaging.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Interfacial Coupling Redirects Biaxial Deformation toward Diffusion-Suppressing Phase Reconstruction in Equimass Poly(3-hydroxybutyrate- co -4-hydroxybutyrate)/Poly(lactic acid) BlendsMacromolecules · 2026
- Influence of PVA Concentration on the Properties of Lontar Palm Leaf‐Sugarcane Bagasse Hybrid Biocomposite FilmsMacromolecular Symposia · 2026
- Development of Biodegradable Talc‐Filled PBAT / PLA and PBSA / PBAT Binary Blend Films: Effects of Multilayer Architecture and Uniaxial Orientation on PerformancePolymer Engineering & Science · 2026
- Toward Compatibility Enhancement of Biodegradable Plasticized Cellulose Acetate and Polyhydroxyalkanoate Blends: Effect of Calcium Carbonate and Maleated Hybrid Blend on Material PerformanceSPE Polymers · 2026
- Comparative Study of Plasticized Polyvinyl Alcohol and Hydroxypropyl Methylcellulose Films for Pharmaceutical Applications: Mechanical, Thermal, Structural and Disintegration PropertiesPolymers · 2026
- Long chain alkyl grafted cellulose and PBST synergistically reinforce PLA: Balanced strength, toughness, and barrier properties.International journal of biological macromolecules · 2026