Rheological, Viscoelastic, and Dynamic Mechanical Behavior of ZnO-Filled and MA-Modified PP/SEBS Filaments for Fused Filament Fabrication.
Chiara das Dores do Nascimento, Everton Granemann Souza, Marcel Luiz Basso, Patricia Oliveira Schmitt, Andre Lamounier Caixeta, Eduarda Vieira Silva, Fabricio Celso, Cesar Aguzzoli,
Graduate Program in Materials Science and Engineering (PPGCEM), Federal University of Pelotas (UFPel), Pelotas, RS 96010-610, Brazil. · Graduate Program in Electronics and Computer Engineering (MEEC), Catholic University of Pelotas (UCPel), Pelotas, RS 96015-560, Brazil.
Key points
From the paper's conclusion- These results demonstrate that MA/ZnO interphase engineering is an effective strategy for improving rheological stability and impact reliability in PP/SEBS filaments for FFF applications.
Abstract
Immiscible polyolefin-elastomer blends often exhibit limited impact resistance and unstable melt-flow behavior due to weak interfacial adhesion and inefficient stress transfer between phases. These limitations are relevant for fused filament fabrication (FFF), where filaments must withstand feeding, extrusion, deposition, and service loading. In this work, PP/SEBS (70/30 wt %) blends modified with maleic anhydride (MA) and ZnO nanoparticles were investigated to determine the influence of interphase engineering on the rheological, viscoelastic, dynamic mechanical, and FFF performance of PP/SEBS filaments. Four formulations (PP/SEBS, PP/SEBS-1%ZnO, PP/SEBS-3%MA, and PP/SEBS-1%ZnO-3%MA) were produced as 1.75 mm filaments and characterized by rotational rheology, DMA, tensile and notched Izod impact tests, SEM, and FTIR. All systems exhibited shear-thinning behavior, while the PP/SEBS-1%ZnO-3%MA formulation showed the most balanced melt response, combining reduced viscosity with adequate viscoelasticity. SEM and DMA analyses suggested improved interphase stability and more efficient viscoelastic dissipation in MA-containing systems. The PP/SEBS-1%ZnO-3%MA blend achieved the highest impact strength (46.86 ± 0.73 kJ m-2), approximately 60% higher than PP/SEBS, while maintaining tensile performance. Preliminary FFF trials demonstrated stable deposition and good dimensional reproducibility. These results demonstrate that MA/ZnO interphase engineering is an effective strategy for improving rheological stability and impact reliability in PP/SEBS filaments for FFF applications.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fused granulate fabrication of short glass fiber-reinforced PA6: Influence of printing parameters on mechanical performance, porosity, and fiber alignmentMaterials & Design · 2025
- Extensional‐Flow‐Controlled Elastomer Dispersion and Toughening in PP / POE Composites During Fused Granulate FabricationJournal of Applied Polymer Science · 2026
- Flexural Behavior of Dual-Material PLA/ABS Specimens Manufactured by Fused Filament Fabrication: Effects of Raster Orientation, Deposition Strategy, and Material CompositionSymmetry · 2026
- Experimental and Numerical Investigation of the Interfacial Bonding in Multi-Material Fused-Filament Fabrication Using Mode-I Fracture Toughness.Polymers · 2026
- Processing-Route Dependence and Adhesion of Polymer-Adhesive-Steel Interfaces with Recycled PA6/GF30 Composites Modified with Functional Additives: Injection Molding Versus Large-Format Fused Granulate Fabrication.Materials (Basel, Switzerland) · 2026
- Large‐Format Fused Granulate Fabrication of Wood‐Filled High‐Density Polyethylene CompositesPolymer Engineering & Science · 2026