ACS omegaOpen accessSpinel

Electrochemical Properties and Changes of Crystal and Electronic Structures of Spinel-Type Mg1.33-y V1.67-x+y Mn x O4 (x = 0.15, 0.06 ≤ y ≤ 0.13) for Magnesium Secondary Batteries.

Yasushi Idemoto, Kohei Yamanouchi, Chiaki Ishibashi, Naoto Kitamura, Toshihiko Mandai, Hidetoshi Somekawa

Department of Pure and Applied Chemistry, Faculty of Science and Technology, Tokyo University of Science, 2641 Yamazaki, Noda-shi, Chiba 278-8510, Japan. · Research Center for Energy and Environmental Materials, National Institute for Materials Science (NIMS), 1-1 Namiki, Tsukuba, Ibaraki 305-0044, Japan.

Key points

From the paper's conclusion
  • The sample with x = 0.15, y = 0.08 had less distortion at the 16d site than the samples with x = 0.15, y = 0.1, and y = 0.13, and the distortion decreased with increasing V content.

Abstract

Mg1.33-y V1.67-x+y Mn x O4 was synthesized by a solid-state method. Powder X-ray diffraction analysis indicated that the product crystallized in the spinel structure with space group Fd3̅m; inductively coupled plasma atomic emission spectroscopic analysis showed that the Mg content was slightly lower than the nominal composition for all samples. Charge-discharge cycle tests showed that the discharge capacity exceeded 180 mAh/g and that the cycle characteristics were reversible up to 20 cycles at 90 °C for the composition with x = 0.15, y = 0.1. The electronic structure was analyzed by the maximum-entropy method on the basis of Rietveld analysis results. The sample with x = 0.15, y = 0.08 had a lower electron density and Mg insertion was easier than in the samples with x = 0.15, y = 0.1, and y = 0.13. The sample with x = 0.15, y = 0.08 had less distortion at the 16d site than the samples with x = 0.15, y = 0.1, and y = 0.13, and the distortion decreased with increasing V content.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers