Corrosion Resistance of Sn-58Bi and Sn-65.7Bi-2.3Sb Low-Melting Alloys in Simulated Geological CO2 Sequestration Environments.
Gonghui Liu, Mengyang Jia, Chunqing Zha, Wei Wang
College of Mechanical and Energy Engineering, Beijing University of Technology, Beijing 100124, China.
Key points
From the paper's conclusion- The study investigates the temperature-dependent corrosion of Sn-58Bi and Sn-65.7Bi-2.3Sb in simulated geological CO2 storage environments.
- When temperature rose from 30 °C to 90 °C, the corrosion-related degradation extent of cement plugs increased from 15.2 mm to 31.6 mm, significantly higher than the increases for Sn-58Bi (0.35 to 0.65 mm) and Sn-65.7Bi-2.3Sb (0.11 to 0.29 mm).
- Sn-65.7Bi-2.3Sb exhibits superior corrosion resistance to Sn-58Bi under simulated CCUS conditions.
Abstract
This study investigates the temperature-dependent corrosion of bismuth-based low-melting alloys (Sn-58Bi and Sn-65.7Bi-2.3Sb) in simulated geological CO2 storage environments. Experiments were conducted in a high-pressure autoclave, with post-corrosion analysis including gas breakthrough tests, digital microscopy, and XPS. Results show that corrosion depth and rate increase with temperature. When temperature rose from 30 °C to 90 °C, the corrosion-related degradation extent of cement plugs increased from 15.2 mm to 31.6 mm, significantly higher than the increases for Sn-58Bi (0.35 to 0.65 mm) and Sn-65.7Bi-2.3Sb (0.11 to 0.29 mm). The degradation mechanisms of the two types of sealing materials were fundamentally different: class G cement plugs mainly experienced CO2-induced bulk degradation within the cement matrix, resulting in structural deterioration, whereas bismuth-based alloy plugs exhibited limited bulk corrosion and were primarily affected by localized degradation at the alloy-casing interface. XPS identified (BiO)2CO3 as the primary corrosion product. Corrosion impaired sealing integrity: after 90 °C exposure, the breakthrough pressure of cement dropped by 73%, compared to only 2.4% for Sn-58Bi and 0.6% for Sn-65.7Bi-2.3Sb. The study concludes that corrosion accelerates with temperature in CO2-rich environments, and Sn-65.7Bi-2.3Sb exhibits superior corrosion resistance to Sn-58Bi, providing experimental insights into the corrosion resistance and sealing performance evolution of these alloys under simulated CCUS conditions.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- The study investigates the temperature-dependent corrosion of Sn-58Bi and Sn-65.7Bi-2.3Sb in simulated geological CO2 storage environments.
- When temperature rose from 30 °C to 90 °C, the corrosion-related degradation extent of cement plugs increased from 15.2 mm to 31.6 mm, significantly higher than the increases for Sn-58Bi (0.35 to 0.65 mm) and Sn-65.7Bi-2.3Sb (0.11 to 0.29 mm).
- Sn-65.7Bi-2.3Sb exhibits superior corrosion resistance to Sn-58Bi under simulated CCUS conditions.
Readers' thoughts
No reader thoughts yet.
Related papers
- Effects of Bi content on melting characteristics, microstructure, and shear strength of Sn-based soldersJournal of Materials Research and Technology · 2025
- Microbial Influence on Corrosive Processes at the Cast Iron-Bentonite Interface during 3.5 Years of Incubation at 37 and 70 °C.Environmental science & technology · 2026
- Corrosion Resistance of Boronized Carbon Steel in a Galinstan-Refrigerant Two-Phase Agitated System.ACS omega · 2026
- Sn-Mediated Regulation of the O₂ Adsorption and Activation Capacity of the Ir/SAPO-34 Catalyst: A Key to Boosting CO Selective Catalytic Reduction of NOₓ in O₂ -Enriched EnvironmentsEnvironmental Science & Technology · 2025
- Weighted Analysis of Corrosion-Inducing Impurities in Supercritical CO2 Transportation System.Molecules (Basel, Switzerland) · 2026
- Analysis of the long-term sealing integrity of cement sheath in CO2 storage wellsScientific Reports · 2026