Influence of Water-Cement Ratio on WPU-Modified Ultrafine Cement Grouting Materials and Reinforcement Mechanism for Crushed Sandstone.
Xiang Cheng, Chaoyu Tian, Yanfen Wang, Guangming Zhao, Yian Chen, Bofang Zhou, Xiangrui Meng, Yingjie Yang
State Key Laboratory of Digital Intelligent Technology for Unmanned Coal Mining, Anhui University of Science and Technology, Huainan, Anhui 232001, China. · School of Materials Science and Engineering, Anhui University of Science and Technology, Huainan, Anhui 232001, China.
Key points
From the paper's conclusion- The results show that the addition of 0.5 wt % WPU shortens the initial setting time, reduces volumetric shrinkage, and enhances mechanical strength.
Abstract
To balance slurry workability for deep-mine grouting and the load-bearing capacity of grouted crushed-sandstone, a waterborne polyurethane (WPU)-modified ultrafine cement composite grouting material was successfully developed using ultrafine Portland cement blended with a polycarboxylate superplasticizer, an expansive agent, and an accelerator. Macro- and microscale characterizations were conducted to clarify the influence of w/c (0.40∼0.60) on slurry properties, mechanical performance, hydration kinetics, and microstructure. Load-bearing behavior and failure modes were further evaluated via crushed sandstone cementation tests. The results show that the addition of 0.5 wt % WPU shortens the initial setting time, reduces volumetric shrinkage, and enhances mechanical strength. With increasing w/c, fluidity and setting time increase markedly, whereas mechanical strength first increases and then decreases. Optimum performance is achieved at a w/c of 0.45, where the 1 d compressive and flexural strengths increase by 22.87 and 4.3%, respectively, relative to the control sample. In the grouting reinforcement test, the 28 d peak strength of the WPU-modified grouted crushed-sandstone specimen at a w/c of 0.45 reaches 20.09 MPa, which is 38.55% higher than that of the control sample, indicating improved load-bearing capacity and elastic deformation capability. XRD, FTIR, SEM, TG, and isothermal calorimetry collectively suggest that the w/c can modulate interfacial coverage and bridging effects of WPU by regulating the water state and pore structure, thereby improving matrix continuity. Accordingly, a triple-coupled mechanism involving hydration-kinetics regulation, interfacial cooperative enhancement, and constrained pore-structure evolution is proposed.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Study on hydration cementation and enhancement mechanism of grout-rock interface of PVA modified grouting material.PloS one · 2026
- Polyurethane Grouting Materials for Mining Applications: Modification Strategies, Performance Trade-Offs, and Engineering ChallengesPolymers · 2026
- Effect of Water Addition on Gel-Forming Capacity and Structure-Property Evolution of Water-Reactive Polyurethane Grout.Polymers · 2026
- Performance evaluation of waste-modified cementitious grouts for cable bolting encapsulationInternational Journal of Geo-Engineering · 2026
- Mechanical Properties and Micro-Mechanism of Polyurethane-Stabilized Calcareous Sand: An Approach for Island Reef ConstructionSustainability · 2026
- Two Component Polyurethane/Epoxy Composite Grouting Material: Injectability, Mechanical Properties, and Engineering ApplicabilityJournal of Applied Polymer Science · 2026