Physicomechanical Properties of a Technical Polyethylene Glycol-Silica-Based Hydrogel as an Alternative Low Shrinkage Dental Polymer Composite.
Abdul Fattah Nongman, Mohd Firdaus Yhaya, Norhafizah Saari, Mariatti Jaafar, Nor Aidaniza Abdul Muttlib, Matheel Zohair Yousif Al-Rawas
Biomaterials Synthesis Laboratory (BSL), School of Dental Sciences, Health Campus, Universiti Sains Malaysia, Kubang Kerian 16150, Kelantan, Malaysia. · Department of Microbiology and Parasitology, School of Medical Sciences, Health Campus, Universiti Sains Malaysia, Kubang Kerian 16150, Kelantan, Malaysia.
Key points
From the paper's conclusion- A synthesized expandable monomer with good polymerization shrinkage properties and the incorporation of silica filler significantly enhanced the mechanical properties compared to pure cured DAPEG 400, with flexural and compressive strengths reaching 10.27 MPa (standard deviation (SD) = 0.96) and 441.42 MPa (SD = 2.80), respectively.
Abstract
Dental composite resins are widely used in restorative dentistry; however, polymerization shrinkage leads to marginal gaps and reduced bond strength. An expandable hydrogel monomer can reduce shrinkage, but it may lack sufficient mechanical strength when used alone. This study developed a low-shrinkage dental composite by incorporating an expandable hydrogel monomer to counteract volumetric shrinkage after curing, aiming to maintain strong bonding to tooth structure. Polyethylene glycol 400 (PEG 400) was chemically modified with acryloyl chloride to produce diacrylated polyethylene glycol 400 (DAPEG 400) expandable hydrogels, which was formulated with silica filler loadings by weight. Statistical analysis involved the Shapiro-Wilk test and one-way ANOVA. A synthesized expandable monomer with good polymerization shrinkage properties and the incorporation of silica filler significantly enhanced the mechanical properties compared to pure cured DAPEG 400, with flexural and compressive strengths reaching 10.27 MPa (standard deviation (SD) = 0.96) and 441.42 MPa (SD = 2.80), respectively. The composite also demonstrated improved dimensional stability, showing 475.32 μg/mm3 (SD = 22.76) reduction in water absorption and 33.37% (SD = 2.26) decrease in volumetric swelling. Most notably, the optimal formulation containing 60% filler exhibited minimal polymerization shrinkage as low as 1.58% (SD = 0.24). The hydrogel's water absorption and expansion after curing offset polymerization contraction, while silica filler regulates expansion to prevent cracking.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Chemical Strategies for Reducing Polymerization Shrinkage Stress in Experimental Dental Resin-Based Materials: A Scoping Review.Dentistry journal · 2026
- The Influence of Filler Morphology and Loading Level on the Properties of Light-Curing Dental CompositesDentistry Journal · 2026
- Measurement of polymerization shrinkage in dental composite resins using a multicolor confocal displacement laser.Dental materials journal · 2026
- Qualification of a Swellable Hydrogel-Silicone Bimorph for Implantable Actuation.Polymers · 2026
- Shrinkage, Degree of Conversion, Water Sorption and Solubility, and Mechanical Properties of Novel One-Shade Universal CompositePolymers · 2025
- The Influence of Polyamide-6 on the Structure and Functional Properties of Composite Hydrogels Based on Polyvinylpyrrolidone Copolymers.Polymers · 2026