Sustainable Synthesis of Diamide Solvents from Succinic Anhydride under Microwave Conditions for the Production of Graphene via Liquid-Phase Exfoliation.
Suphatta Aintharabunya, Suwiwat Sangon, Yuvarat Ngernyen, Francesca M Kerton, Christopher M Kozak, James Sherwood, Nontipa Supanchaiyamat, Andrew J Hunt
Materials Chemistry Research Center, Department of Chemistry and Center of Excellence for Innovation in Chemistry, Faculty of Science, Khon Kaen University, Khon Kaen 40002, Thailand. · Department of Chemical Engineering, Faculty of Engineering, Khon Kaen University, Khon Kaen 40002, Thailand.
Key points
From the paper's conclusion- Liquid-phase exfoliation (LPE) is a viable method for the large-scale production of two-dimensional (2D) graphene; however, toxic solvents must be replaced.
Abstract
Liquid-phase exfoliation (LPE) is a viable method for the large-scale production of two-dimensional (2D) graphene; however, toxic solvents must be replaced. The microwave synthesis of sustainable succindiamide solvents, namely N,N'-diethyl-N,N'-dibutylsuccindiamide (EBSA) and N,N,N',N'-tetrabutylsuccindiamide (TBSA), was investigated and applied to the LPE of graphite to obtain graphene. The yield of EBSA was 99.4% from succinic anhydride with a K60 silica gel catalyst under microwave conditions (160 °C in 30 min), while TBSA presented an 88.8% yield at 180 °C. The green metric demonstrated that this route has a significantly lower Process Mass Intensity (PMI) and higher Reaction Mass Efficiency (RME) values compared to previously published routes. TBSA demonstrated a ∼150% increase in the graphene and graphene oxide exfoliation (thickness <7 nm) compared to N-methylpyrrolidone (NMP). TBSA outperformed Cyrene in the LPE of graphene oxide. Graphene and graphene oxide nanosheets were characterized by transmission electron microscopy (TEM), Raman spectroscopy, X-ray diffraction (XRD), and atomic force microscopy (AFM). The solvent surface tension, density, viscosity, Hansen Solubility Parameters (HSPs), and Kamlet-Abboud-Taft parameters (KATs) were investigated to determine the key parameters for exfoliation. The high dipolarity (π*) and hydrogen bond-accepting ability (β) of TBSA promoted significant graphene exfoliation, while its greater viscosity produced high-quality graphene sheets, with I D/I G ratios of 0.005 ± 0.02 for graphene flakes of <1 μm. Higher-viscosity solvents demonstrated a limited increase in the graphene concentration with longer sonication, but retained high-quality graphene. TBSA is a potentially greener alternative to NMP for LPE, leading to opportunities for sustainable graphene production.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Sustainable Synthesis of Few‐Layer Graphene From Waste Fuel Cell Plates via Lysine‐Assisted Ball Milling for Solar DesalinationAdvanced Sustainable Systems · 2026
- Scalable Nondestructive Exfoliation of Layered Materials Into Monolayers via Shear-Transducing Interfaces.Advanced materials (Deerfield Beach, Fla.) · 2026
- Achieving high-yield and pilot-scale synthesis of nano graphene oxide via photochemical defect engineering and oxidative cleavageNature Communications · 2026
- Graphene-Oxide-Based Organic Solvent Filtration Membranes: Recent Progress and Perspectives.Chem & bio engineering · 2026
- Green strategies for MXene synthesis: Toward sustainable nanomaterials and emerging applicationsResults in Engineering · 2026
- Solvent‐Based Chemical Delamination of End‐Of‐Life Photovoltaic Modules: A Systematic ReviewSolar RRL · 2026