From the paper's conclusion- It was found that the EDAC/NHS treatment improved the mechanical strength and biostability of the chitosan–fish scale collagen 3D porous architecture in the presence of glycerin and enhanced the cytocompatibility of scaffolds.
Abstract
The three-dimensional porous architecture of scaffolds strongly influences cell infiltration and cell-cell and cell-matrix interactions. The mechanical strength and biostability of three-dimensional (3D) porous scaffolds remain challenges for maintaining the 3D porous architecture and facilitating cell infiltration and cell-cell and cell-matrix interactions. In this study, the mechanical strength and biostability of chitosan-fish scale collagen 3D porous scaffolds were improved by using EDAC/NHS cross-linking in the presence of glycerin. Furthermore, the microstructure, physicochemical properties, mechanical strength, biostability, and cytocompatibility of the scaffolds were investigated. Chitosan-fish scale collagen/glycerin 3D porous scaffolds were fabricated via the EDAC/NHS cross-linking. Cross-linking effects on scaffold microstructures and physicochemical properties were investigated, while the scaffolds' mechanical strength and biostability were determined by using mechanical and biodegradation tests. Cytocompatibility tests were used to explore the ability of 3D porous scaffolds to be used for tissue engineering applications. The scaffolds' cross-linking density/degree, tensile modulus, and biostability were increased and pore size decreased with EDAC/NHS cross-linking treatment, resulting in enhanced mechanical strength and biostability of the 3D porous architecture of the scaffolds. The average tensile modulus of the cross-linking scaffold in a dry environment was in a range of 4.61 ± 2.33-0.62 ± 0.13 MPa, with a tensile modulus in a wet environment of 25.2 ± 6.32-17.74 ± 6.00 KPa, a biodegradation rate at day 30 of 28.73 ± 4.58-26.014 ± 1.70, and average pore sizes of 151.33 ± 53.66-142.31 ± 60.67 μm. In vitro culture of human fibroblasts and keratinocytes showed that the mechanical strength and biostability of cross-linking scaffolds supported cell proliferation, adhesion, spreading, and infiltration. It was found that the EDAC/NHS treatment improved the mechanical strength and biostability of the chitosan-fish scale collagen 3D porous architecture in the presence of glycerin and enhanced the cytocompatibility of scaffolds.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Insights into Schiff-base crosslinking in chitosan porous scaffolds: the role of dialdehyde polysaccharide ionic nature and bioactive functionalization.Journal of materials chemistry. B · 2026
- Investigating the crosslinking of an aligned, all-natural chitosan-gelatine-cellulose based polymeric scaffold for tendon tissue engineeringBiomaterials Advances · 2026
- Recent Advances and Applications of Chitin and Chitosan Hydrogel Scaffolds in Tissue EngineeringGels · 2026
- Surface modification of 3D-printed polycaprolactone scaffolds with silk fibroin for bone tissue engineering.FEBS open bio · 2026
- Croaker Fish Bone-Derived Hydroxyapatite as a Sustainable Source for 3D-Printed Scaffolds for Bone Regeneration.Marine drugs · 2026
- 3D-printed core–shell scaffolds with a biphasic calcium phosphate core and GelMA hydrogel shell for bone tissue engineeringScientific Reports · 2026