Dose-Dependent and Irreversible Photodarkening of InP/ZnSe/ZnS Quantum Dots
Raimon Terricabres-Polo, Reinout F. Ubbink, Erik Betz-Güttner, Freddy T. Rabouw, Arjan J. Houtepen, Celso de Mello Donegá
Utrecht University · Optoelectronica-2001 (Romania)
Key points
From the paper's conclusion- These findings advance understanding of InP-based QD photodegradation and provide a framework for quantifying their stability under light stress.
Abstract
Indium phosphide-based quantum dots (QDs) are leading Cd- and Pb-free alternatives for photonic applications spanning 400–920 nm. However, their long-term photostability under prolonged illumination remains poorly understood. In this study, we systematically investigate the optical response of colloidal InP/ZnSe/ZnS core/shell/shell QDs exposed to white light under a dynamic inert atmosphere (glovebox filled with circulating N 2 with O 2 < 0.1 ppm, H 2 O < 1.0 ppm). Upon illumination, the QDs exhibit irreversible photodarkening, defined as a reduction in photoluminescence quantum yield with a nearly unchanged absorption spectrum. Photodarkening shows a linear dependence on absorbed photon dose, with photoexcitation deep into the conduction band inducing it more rapidly than resonant photoexcitation. Additionally, prolonged photoexposure leads to an emission redshift and an enhanced delayed-emission component, consistent with the selective photodarkening of individual QDs. Experiments in air and controlled humidity (10% and 90% relative humidity) indicate that photodarkening primarily arises from photooxidation by oxygen, whereas water promotes QD photoetching. This is further corroborated by control experiments in which the QDs are illuminated under dry oxygen (<3 ppm of H 2 O) and in a cuvette sealed by fusion under a N 2 atmosphere with <0.1 ppm of O 2 and <1 ppm of H 2 O. These experiments show that photodarkening does not occur in QDs contained in the fusion-sealed cuvette, while under dry oxygen the photodarkening rates of the QDs are even faster than in dry air. These findings advance understanding of InP-based QD photodegradation and provide a framework for quantifying their stability under light stress.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Photoquenching-by-Photocharging: A Single Process of Failure of Oxygen-Exposed InP/ZnSe Quantum DotsACS Nano · 2026
- Controlled Surface Ga Treatment to Suppress the Ostwald Ripening Process for InP Quantum Dots with Narrow-Bandwidth Emission.Langmuir : the ACS journal of surfaces and colloids · 2026
- Indium Phosphide Quantum Dots for Near-Infrared Luminescence-Based Bioimaging and Theranostics: From Photophysical Design to Clinical Translation.Luminescence : the journal of biological and chemical luminescence · 2026
- Pre-Shell Protection Suppresses Facet-Selective Core Digestion in InP Quantum Dots for High-Yield and Uniform Core/Shell StructuresACS Applied Materials & Interfaces · 2025
- Indium Phosphide Quantum Dots in Biomedicine: Photophysics, Bio-Nano Interactions, and Emerging Imaging and Therapeutic Platforms.Luminescence : the journal of biological and chemical luminescence · 2026
- Thermal and chemical control of emission and excited-state dynamics in non-(TMS)3P-derived InP quantum dotsThe Journal of Chemical Physics · 2026