Solid-State Chemical Recycling of Anhydride-Based Polymers: From Linear Copolyesters to Cross-Linked Epoxy Networks.
Guo-Xu Wang, Xiang Li, Yu-Hao Zhang, Hao-Yun Liu, Ze-Hua Liu, Bai-Hao Ren, Qing Liu, Qiu-Yu Zhang,
School of Chemistry and Chemical Engineering, Key Laboratory of Special Functional and Smart Polymer Materials of Ministry of Industry and Information Technology, Northwestern Polytechnical University, Xi'an, 710072, China. · Department of Chemistry and Chemical Biology, Baker Laboratory, Cornell University, Ithaca, New York 14853-1301, United States; State Key Laboratory of Fine Chemicals, Frontiers Science Center for Smart Materials, Dalian University of Technology, Dalian, 116024, China.
Key points
From the paper's conclusion- Notably, DPMA-based epoxy resins exhibit attractive thermomechanical performance, with glass transition temperatures spanning 101-136 °C and a tensile strength at break of ∼74.7 MPa, while retaining efficient closed-loop chemical recyclability.
Abstract
Chemical recycling of polymers to the parent monomers (CRM) represents a cornerstone strategy for establishing a sustainable circular plastic economy. Polyesters prepared by ring-opening copolymerization of epoxides with cyclic anhydrides feature highly tunable properties and represent promising alternatives to petroleum-derived polymers. Nevertheless, direct and selective chemical recycling of such copolyesters into pristine monomers continues to pose a substantial challenge. Herein, we report a versatile and highly efficient strategy for the solid-state depolymerization of both linear copolyesters and cross-linked epoxy networks derived from diphenylmaleic anhydride (DPMA) and epoxides. The depolymerization process is catalyzed by ZnCl2 via a random chain-scission mechanism, delivering exceptional DPMA selectivity (>99%) and high recovery yield (≥85%). Combined mechanistic investigations and density functional theory (DFT) calculations elucidate a stepwise depolymerization route involving spirolactone intermediates as critical species. Notably, DPMA-based epoxy resins exhibit attractive thermomechanical performance, with glass transition temperatures spanning 101-136 °C and a tensile strength at break of ∼74.7 MPa, while retaining efficient closed-loop chemical recyclability. This work thus establishes a reliable platform for the rational design of high-performance polymer materials that integrate robust mechanical properties with fully reversible chemical recycling.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Direct metathesis deconstruction to recycle poly(dicyclopentadiene) composites.Science advances · 2026
- Lifecycle of dynamic covalent polar-olefin macrocycles via entropy-driven ring-opening polymerization and closed-loop chemical recyclingNational Science Review · 2025
- Mechanically Triggered Chemical Recyclable Polyethylene‐Like MaterialsAngewandte Chemie International Edition · 2026
- Benzo-Fused Monomer Design toward Semiaromatic Polymers for a Circular Plastic EconomyAccounts of Chemical Research · 2026
- Chemically Recyclable Polymers: Tunable Performance Enabled by Precision Ring-Opening (Co)polymerization.Precision chemistry · 2026
- Dynamic Diels-Alder Chemistry Toward Degradable and Dual Closed-Loop Recyclable Polyolefins.Angewandte Chemie (International ed. in English) · 2026