ACS Energy Letters

Prestripping Protocol for Reconciling Lithium Dissolution and Galvanic Corrosion in Anode-Free Batteries

Tianyang Yu, Teng Zhao, Xue Pang, Ke Wang, Wangming Tang, Li Li, Renjie Chen

Key points

From the paper's conclusion
  • Here, we introduce a pre-stripping protocol consisting of a brief low-current stripping step followed immediately by higher-current bulk stripping, thereby establishing a uniform initial dissolution front while limiting the duration of Li–Cu galvanic coupling.

Abstract

The practical viability of high-energy-density anode-free lithium metal batteries is limited by the poor reversibility of lithium plating and stripping. Low-current stripping suppresses pitting and inactive Li formation but prolongs electrolyte exposure and galvanic corrosion, whereas high-current stripping shortens the corrosion time but promotes localized dissolution and structural disintegration. Here, we introduce a pre-stripping protocol consisting of a brief low-current stripping step followed immediately by higher-current bulk stripping, thereby establishing a uniform initial dissolution front while limiting the duration of Li–Cu galvanic coupling. Measurements across representative electrolyte formulations identify three factors associated with the balance between morphological regulation and corrosion loss: nascent solid electrolyte interphase (SEI) passivation, longer-term corrosion tolerance, and dynamic reaction area evolution. In strongly passivating formulations, the morphological benefit of prestripping outweighs the additional corrosion loss and improves Li reversibility. The protocol was further evaluated in 1 Ah anode-free pouch cells, supporting its applicability to practical cell configurations.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers