Multiple Synergistic Effects of Different Stretching and Heating Fields on the Structure Evolution and α′-to-α Transition of PA66 Fibers during Melt Spinning
Wei-Xin Wu, Xian-Ning Shi, Bo Wang, Ze-Tian Zhang, Shuang-You Shi, Yong-Ming Shi, Zong-Zi Hou, Peng-Fei Wu
Key points
From the paper's conclusion- This study constructed a structure–property model of PA66 fibers under different drawing processes, providing a theoretical basis for high-performance polyamide fibers.
Abstract
This study prepared high-strength, low-elongation PA66 fibers (tensile strength ∼ 10.14 cN/dtex, elongation ∼ 10.5%) via high-speed one-step melt spinning combined with two-stage drawing and heat setting, achieving a maximum draw ratio exceeding 5.5. Using 2D-SAXS/WAXS and FTIR, the competitive multiscale structural evolution of PA66 fibers under thermal and tensile-stress driving was systematically investigated, covering microstructure (crystal transition, chain conformation, hydrogen bonding), submicrostructure (long period and orientation), and macroscopic mechanical properties; and a three-phase structure and crystal-transition model was established. Drawing and heat setting promoted the breaking of irregular hydrogen bonds and the reconstruction of ordered ones, accompanied by lattice deformation and trans-conformation recovery. Both L-PA66 and H-PA66 fibers exhibited an α′-to-α crystal transition; H-PA66 fibers showed a higher crystal transition temperature (ST = 250 °C) and insignificant Poisson contraction due to their high orientation and compact chain conformation. Under high stress, MAF in H-PA66 fibers gradually transformed into RAF, giving a more perfect and uniform structure with markedly enhanced orientation; fibrillar crystals grew along the (010)/(110) planes, the grains were refined, and crystallinity and mechanical properties improved significantly. L-PA66 fibers tended toward thermally controlled equilibrium relaxation due to H-DT; although the crystalline region gradually became more perfect and partially compensated for amorphous deorientation, deorientation driven by higher ST (230 °C < T < 250 °C) remained unavoidable. This study constructed a structure–property model of PA66 fibers under different drawing processes, providing a theoretical basis for high-performance polyamide fibers.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Geometric Freezing of In-Situ Fibrillated PP/PA66 Composites via Low-Temperature Injection: Decoupling the Role of Draw Ratio and Compatibilization.Polymers · 2026
- Fabrication of high-strength collagen fibers via a novel integrated liquid crystal and microfluidic spinning.International journal of biological macromolecules · 2026
- In Situ Polycondensation for Rigid–Flexible Nanofibrillar Composites of Aramid Nanofibers and Polyamide 66ACS Applied Polymer Materials · 2026
- Stable Helical Crimp Formation in PET / PA6 Bicomponent Filaments via Hygrothermally Enhanced Shrinkage MismatchJournal of Applied Polymer Science · 2026
- Additive Manufacturing of Polyamide-6 Preforms for Scalable Thermal Drawing of Structured Fibers.Micromachines · 2026
- Tailoring the Mechanical Properties of L‐DED‐Fabricated γ‐TiAl Alloys Through Heat Treatment: Correlating Microstructural Evolution With Fracture MechanismsRare Metals · 2026