From the paper's conclusion- Two series of sulfonated polyaromatic polymers were synthesized via a facile superacid polycondensation followed by postsulfonation, one bearing nonsulfonable ethyl side chains and the other sulfonable phenyl side chains.
- The ethyl side chain-based polymer exhibited higher proton conductivity and superior dimensional stability.
- The phenyl side chain-based PEM suffered severe edge cracking at the membrane/porous transport layer interface after accelerated stress testing, caused by excessive swelling.
Abstract
Abstract The pursuit of durable and high-performance proton exchange membranes via rational molecular design is crucial for advancing green hydrogen production through water electrolysis. Two series of sulfonated polyaromatic polymers were synthesized via a facile superacid polycondensation followed by postsulfonation, one bearing nonsulfonable ethyl side chains and the other sulfonable phenyl side chains. Morphological characterizations confirmed distinct hydrophilic/hydrophobic phase separation in the ethyl side chain-based sulfonated polyaromatic polymer with an ion exchange capacity of 2.08 mmol g–1. Compared to its phenyl side chain-based counterpart with an ion exchange capacity of 1.99 mmol g–1, the ethyl side chain-based polymer exhibited higher proton conductivity and superior dimensional stability. The membrane electrode assembly based on the polymer with nonsulfonable spacers delivered excellent electrolysis polarization performance and robust durability. The phenyl side chain-based PEM suffered severe edge cracking at the membrane/porous transport layer interface after accelerated stress testing, caused by excessive swelling.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- Two series of sulfonated polyaromatic polymers were synthesized via a facile superacid polycondensation followed by postsulfonation, one bearing nonsulfonable ethyl side chains and the other sulfonable phenyl side chains.
- The ethyl side chain-based polymer exhibited higher proton conductivity and superior dimensional stability.
- The phenyl side chain-based PEM suffered severe edge cracking at the membrane/porous transport layer interface after accelerated stress testing, caused by excessive swelling.
Readers' thoughts
No reader thoughts yet.
Related papers
- Structural Design and Performance Optimization of Proton Exchange Membranes for Water Electrolysis: A ReviewMembranes · 2026
- Synergistic Enhancement of Proton Conductivity in Proton Exchange Membranes via Acid–Base Cross-Linked Dual Proton ChannelsACS Applied Polymer Materials · 2025
- Tailoring Backbone Geometry Via Positional Isomerism in Poly(carbazole)-Based Proton Exchange Membranes with High Conductivity and Dimensional Stability for Water Electrolysis and Fuel CellsMacromolecules · 2026
- Towards Sustainable Proton Exchange Membranes: Materials and Challenges for Water ElectrolysisWater · 2025
- Mechanically Reinforced Anion-Exchange Composite Membrane with Improved Interface Integrity for Water ElectrolysisMembranes · 2026
- Structure-Property Relationship of Dialkyl and Spirocyclic Piperidinium based Poly(biphenyl piperidinium) Anion Exchange MembranesNewcastle University ePrints (Newcastle Univesity) · 2026