Composition-Driven Phase Separation, Micellar Ordering, and Sulfadiazine Release in Poly(vinylpyrrolidone)-Tetronic 908 Hydrogels.
Hanan Rafid Al-Taha, Gustavo González-Gaitano, Gregory N Smith, Javier González-Benito, Margarita Valero
Departamento Química Física, Facultad de Farmacia, Universidad de Salamanca, Campus Miguel de Unamuno, s/n, 37007 Salamanca, Spain. · Departamento de Química, Universidad de Navarra, 31080 Pamplona, Spain.
Key points
From the paper's conclusion- We investigate the phase behavior, nanostructure, swelling, and sulfadiazine (SDZ) release of aqueous PVP K90-Tetronic 908 (T908) blends with concentration and T908:PVP ratio.
Abstract
We investigate the phase behavior, nanostructure, swelling, and sulfadiazine (SDZ) release of aqueous PVP K90-Tetronic 908 (T908) blends with concentration and T908:PVP ratio. Phase diagrams (20 °C-80 °C, 5-30 wt %) reveal a percolation threshold at ∼25 wt %: below it, mixtures form clear solutions or coexisting liquid phases; above it, a gel forms at physiological temperature. Phase coexistencedemixing into a T908-rich clear liquid and a PVP-rich turbid phase, with T908 inserted into the PVP networkoccurs across most compositions at low temperature (20 °C-35 °C), and persists across the full range (20 °C-80 °C) near 1:1 T908:PVP ratios; there, the PVP-rich phase is dense and cohesive, liquid at low temperature and gelling upon heating. Small-angle neutron scattering (SANS) supports this picture at the nanoscale: individual micelle size is largely unaffected by PVP content. In the T15:P15 blend, T908 forms free micelles at 20 °Cwhere a low-q upturn confirms nanoscale microsegregationand a body-centered cubic (BCC) gel at 37 °C; however, only part of the nominal 15 wt % T908 enters the ordered BCC lattice: 15 wt % alone is insufficient for gelation, but local crowding in the PVP-rich domain raises T908 above this threshold there. The remaining T908 likely resides in the coexisting T908-rich liquid phase, below its local aggregation concentration, as unimers rather than micelles. Swelling and SDZ release both reflect this phase-separated architecture, though not proportionally: T908 substantially enhances water uptake versus pure PVP, but blend swelling is nonadditive, and the 1:1 (w/w) blenddespite lower net swelling than pure T908released more SDZ per gram (0.12 ± 0.04 mgSDZ/gformulation) than the 5:1 blend (0.083 ± 0.011 mgSDZ/gformulation) or pure PVP (0.068 ± 0.006 mgSDZ/gformulation), pointing to the dense phase as a preferential drug reservoir.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Unlocking the Potential of Poloxamine 908 for Injectable Nanocomposite Hydrogels: Rheological Performance, Dissolution Behavior and Sustained Drug Release.Pharmaceutics · 2026
- Nanogels with volume phase transition for biomedical applicationsNature Communications · 2025
- Decoupled Attraction and Repulsion for Fast, Large, and Reversible Thermal Actuation in Hydrogels.ACS applied materials & interfaces · 2026
- Multi‐scale Engineered Vasculature and Hierarchical Porosity via Volumetric Bioprinting‐Guided Photopolymerization‐Induced Phase SeparationAdvanced Materials · 2025
- Controlling Polymerization-Induced Phase Separation in the Synthesis of Porous GelsACS Nano · 2025
- Investigating the roles of hydrophobicity and electrostatics in the particle-scale dynamics and rheology of dense microgel suspensionsJournal of Applied Physics · 2026