  • Structural degradation, known as a real bottleneck on reversible ion intercalation in the cathodes, was addressed by using todorokite manganese dioxide (t-MnO2).

Abstract

Augmenting mechanical sturdiness while hindering zinc-dendrite initiation and diminishing electrolyte-related degradation remains at the leading edge of developing high-performance aqueous zinc-ion batteries (AZIBs). Herein, not only is the preservation of zinc anodes against dendrite formation achieved, but also acceleration of zinc-ion transport is obtained through grafting defect-rich zinc-based metal organic frameworks (DR-Zn MOFs) onto zinc anodes. Direct growth of missing linker DR-Zn MOFs onto the anodes was accomplished, employing a modulation strategy that integrates isophthalic acid (IPA) into the trimesic acid (H3BTC) linkers. The arrayed DR-Zn MOFs onto the zinc foils can effectively suppress the hydrogen evolution reaction (HER), elevate the corrosion potential by +0.06 V, and mitigate zinc dendrite growth. Uniform ionic and electric field distributions significantly enhance the cycle stability of DR-Zn MOF-protected anodes compared to bare counterparts, extending operation from 88 h to over 500 h at 4 mA cm−2. Structural degradation, known as a real bottleneck on reversible ion intercalation in the cathodes, was addressed by using todorokite manganese dioxide (t-MnO2). Tunneled-structure t-MnO2 exhibits not only long cycle stability but also enhanced ion storage, achieving a discharge capacity of 53.70 mAh g−1 at 0.5 mA cm−2, compared with 37.55 mAh g−1 for α-MnO2. Finally, the DR-Zn MOF-treated anodes paired with t-MnO2 cathodes in AZIB full cells achieved a specific capacity of 400.4 mAh g−1 at 0.2 A g−1, while exhibiting remarkable cycle stability with a minimal capacity fade of 0.02% per cycle and preserving over 79.6% of initial capacity after 1000 cycles at a fixed current density of 1 A g−1.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers