Key Laboratory of Photochemical Conversion and Optoelectronic Materials, Technical Institute of Physics and Chemistry, University of Chinese Academy of Sciences, Chinese Academy of Sciences, Beijing100190, China. · Key Laboratory of Photochemistry, Institute of Chemistry, University of Chinese Academy of Sciences, Chinese Academy of Sciences, Beijing100190, China.
Key points
From the paper's conclusion- By tuning the molecular weight of PoMA, we optimized the delicate balance between sensitivity and resolution, achieving 18 nm half-pitch (HP) resolution with a line edge roughness (LER) of 1.7 nm in electron beam lithography (EBL) and 30 nm HP with 2.5 nm LER in EUVL.
Abstract
The transition to high-numerical-aperture (High-NA) extreme ultraviolet lithography (EUVL) imposes stringent constraints on resist film thickness, posing a critical challenge in terms of maintaining film thickness consistency to ensure pattern fidelity during subsequent etching processes. Herein, we introduce a molecular design strategy that intrinsically addresses this issue by employing an atom-conservative photochemical reaction. A series of non-chemically amplified resists (n-CARs) based on ortho-nitrobenzaldehyde (o-NBA)-modified PMMA polymers (PoMA) were developed. Distinct from conventional resists that suffer from decomposition-induced thickness loss, PoMA leverages a unique intramolecular rearrangement mechanism. Upon exposure, the o-NBA moieties undergo an intramolecular photorearrangement into ortho-nitrosobenzoic acid (o-NSBA), inducing a polarity switch for negative-tone development (NTD) without mass loss. Consequently, the PoMA resists exhibited near-quantitative film retention after exposure and development. By tuning the molecular weight of PoMA, we optimized the delicate balance between sensitivity and resolution, achieving 18 nm half-pitch (HP) resolution with a line edge roughness (LER) of 1.7 nm in electron beam lithography (EBL) and 30 nm HP with 2.5 nm LER in EUVL. Furthermore, etch resistance and pattern transfer capability into silicon at feature sizes down to 25 nm HP were also demonstrated. These findings highlight the atom-economic rearrangement strategy as a promising paradigm for designing photoresists for advanced lithography, effectively addressing the critical issue of film thickness loss in ultrathin resist layers.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Recent Progress of Nonchemically‐Amplified Resists for High‐Resolution Lithography†Chinese Journal of Chemistry · 2026
- Revealing Structure-Driven Performance of Molecular-Atomic Layer Deposited Resists for Extreme Ultraviolet Lithography through In Situ Analysis.ACS nano · 2026
- Molecular nonchemically amplified resists based on spirobixanthene backbone: Sulfoxime oxime esters versus sulfonium saltsSmart Molecules · 2025
- Designing Stable Photoresists Using Polymers With Photoinduced Reversible Solid-to-Liquid Transitions for Nanoimprint Lithography.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Polarity‐engineered Sn‐Ti cluster photoresists for sub‐10‐nm high‐resolution lithographySmart Molecules · 2026
- Positive and Negative Dual-Type Hafnium-Based Hybrid Dry Photoresist for NanolithographyACS Applied Materials & Interfaces · 2026