ACS applied materials & interfaces

Quantifying the Heterointerface Contribution in a Cu7S4/CuCo2S4 Cathode with LiCl-All-Phenyl Complex Electrolyte for High-Performance Magnesium/Lithium Hybrid-Ion Batteries.

Xuehui Wang, Guangwu Zhang, Kaifeng Huang, Xiang Fang, Cheng Wang, Haojun Xu, Chenchen Zhang, Xiaoya Wang,

Key Laboratory of Functional Molecular Solids, Ministry of Education, College of Chemistry and Materials Science, Anhui Normal University, Wuhu, Anhui241002, P.R. China. · Department of Mechanical and Aerospace Engineering, The Hong Kong University of Science and Technology, Hong Kong SAR999077, P.R. China.

Computational

Key points

From the paper's conclusion
  • Here, we construct a Cu7S4/CuCo2S4 heterostructure in a single hydrothermal process, in which the two phases sharing a common Cu–S sublattice form a coherent interface within individual particles.

Abstract

Heterostructured cathodes are widely credited with accelerating conversion kinetics in magnesium/lithium hybrid-ion batteries (MLHBs). Here, we construct a Cu7S4/CuCo2S4 heterostructure in a single hydrothermal process, in which the two phases sharing a common Cu-S sublattice form a coherent interface within individual particles. By fixing the phase ratio independently through Rietveld refinement and benchmarking against both phase-pure constituents under identical conditions, we show that the composite exceeds the composition-weighted rule-of-mixtures prediction by a factor of 3.4 at 0.3 A g-1. Because the constituents exhibit closely comparable charge-discharge profiles, the redox chemistry itself is unchanged, and this strongly super-additive response can primarily originate from the interface rather than from composition. Elemental mapping and surface-sensitive XPS, together with the coexistence of Li2S and MgS in in situ XRD, further reveal that storage is spatially partitioned: Li+ converts the particle interior while Mg2+ reacts predominantly in the near-surface region, so that the two carriers occupy complementary regions of the same particle. Comparing APC-LiCl with APC-LiTFSI at matched salt concentration, and identical in every other respect, localizes the electrolyte effect to the electrode interface, where the chloride-containing system suppresses the progressive Mg-surface passivation that drives continuous overpotential growth in the TFSI- system. The resulting cell delivers 400 mAh g-1 at 0.3 A g-1 and retains 152.56 mAh g-1 after 330 cycles at 1.0 A g-1 at ∼100% Coulombic efficiency. DFT calculations indicate increased states near the Fermi level and a localized interfacial electrostatic gradient consistent with the measured kinetics.