Probing the Hidden Interfaces in Cr-LiF Conversion Cathodes in Thin-Film Solid-State Batteries.
Vittorio Montanelli, Joel Casella, Jędrzej Morzy, Stefano Saroglia, Rolf Erni, Yaroslav E Romanyuk, Marta D Rossell
Electron Microscopy Center, Empa, Swiss Federal Laboratories for Materials Science and Technology, Dübendorf8600, Switzerland. · Laboratory for Thin Films and Photovoltaics, Empa, Swiss Federal Laboratories for Materials Science and Technology, Dübendorf8600, Switzerland.
Key points
From the paper's conclusion- Our results show that the capacity decay in Cr-LiF cathodes is dominated by self-limiting interfacial degradation, underscoring interface engineering as the critical strategy for advancing high-performance conversion-type solid-state batteries.
Abstract
Conversion cathodes based on transition metal fluorides enable multi-electron redox reactions and high theoretical energy densities, making them promising candidates for next-generation solid-state batteries. Here, we elucidate the nanoscale structural, chemical, and redox evolution of Cr-LiF conversion cathodes integrated into thin-film solid-state batteries with a LiPON solid electrolyte using advanced transmission electron microscopy. Comparison of the discharged and charged states reveals a reversible Cr0/Cr2+ redox process mediated by CrF2 formation, while no evidence of higher chromium oxidation states is observed under operating conditions. We identify the formation of a Cr3+-rich cathode-electrolyte interphase composed primarily of a mixed CrOxNy phase and reveal pronounced cycling-induced compositional gradients and interfacial transformations. Extended cycling promotes Ti diffusion from the current collector into the cathode, leading to the formation of TiOF2/TiFx species that scavenge fluoride and locally deplete lithium. Together, these interfacial reactions reduce the fraction of electrochemically active cathode material, causing an initial capacity fade that subsequently stabilizes with cycling while largely preserving charge transport. Our results show that the capacity decay in Cr-LiF cathodes is dominated by self-limiting interfacial degradation, underscoring interface engineering as the critical strategy for advancing high-performance conversion-type solid-state batteries.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Review on Cathode‐Electrolyte Interphase for Stabilizing Interfaces in Solid‐State Lithium BatteriesAdvanced Science · 2025
- Ultrafast Electron–Ion Transport in Micron-Scale Iron Difluoride Cathode by Self-Assembly of Nanoconfined Carbon BlackACS Applied Nano Materials · 2026
- Understanding the Multi‐Electron Conversion Mechanism and High Performance of NbCl 5 Cathodes in All‐Solid‐State Lithium BatteriesAdvanced Functional Materials · 2026
- Recent Progress in Solid‐State Lithium Batteries through Cathode Microstructure EngineeringAdvanced Science · 2025
- Visualizing a Li-Depleted Amorphous Cathode-Electrolyte Interphase in Sulfide Solid-State Batteries Using In Situ Cryogenic Electron Microscopy.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026
- Compositionally Tuned LiFeO2–LiCoO2–LiNi0.5Mn0.5O2 Cathodes for All-Solid-State Lithium Batteries: Cathode–Solid Electrolyte Interactions and Energy-Density ConsiderationsInorganics · 2026