Crystallinity-Dependent Donor Activation in RF-Sputtered SnO2 Electron-Transport Layers and the Interface-Character Origin of Their Predicted Device-Level Consequences.
Ji-Seong Hwang, Soo Min Kim, Yoonmook Kang
Department of Materials Science and Engineering, Korea University, Seoul02841, Republic of Korea. · Nano Convergence Materials Center, Emerging Materials R&D Division, Korea Institute of Ceramic Engineering and Technology (KICET), Jinju52851, Republic of Korea.
Key points
From the paper's conclusion- The predicted crystallization gain is +5.6 pp (20.5 → 26.1%).
Abstract
SnO2 is the electron-transport layer (ETL) in record n-i-p perovskite solar cells, grown by chemical bath deposition (CBD) without high-temperature crystallization; whether its crystallinity matters remains unresolved. Here, the same RF-sputtering process on fluorine-doped tin oxide (FTO), at room temperature or 300 °C, yields a predominantly amorphous or an FTO-templated polycrystalline rutile film. The measured film and interface properties anchor a calibrated TCAD model and a thirteen-parameter Sobol global sensitivity analysis (>33,000 simulations), which, unlike one-factor-at-a-time sweeps, resolves the interactions among parameters explicitly. At the film level, crystallinity governs donor activation: UPS, XPS, and STEM-EDS show that the amorphous film holds more fluorine yet has a Fermi level farther below the conduction band, so shallow donors attributed to substitutional fluorine exist in both films but are active only in the crystalline one. At the device level, however, the predicted gain arises from the crystalline film's interface rather than its doping. The Ag/SnO2 contact is rectifying on the amorphous film and ohmic on the crystalline one, through interface-state de-pinning rather than a band-offset shift. The Sobol analysis ranks the SnO2/perovskite interface trap density first (total-effect index ≈ 0.66). A degenerately doped film could screen such traps, but the amorphous film's rectification rules out that route; its deficit is interfacial. At its trap density (∼1013 cm-2), only deep acceptor-like states pin the Fermi level (acceptor-fraction index ≈ 0.83). The predicted crystallization gain is +5.6 pp (20.5 → 26.1%). FAPbI3 half-stack PL/TRPL supports this (1.35× longer lifetime on the crystalline ETL) and bounds that interface's trap density to ≲1012 cm-2. Crystalline growth is one route to the de-pinned interface that CBD ETLs reach chemically, provided that interface is preserved. The absolute efficiencies are calibrated predictions; the benefit's sign and the lever ranking are robust.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Optimized SnO₂ Thin Films: Correlating Solution Chemistry and Deposition Conditions with Optoelectronic PropertiesACS Applied Materials & Interfaces · 2026
- Ozone Treatment of SnO₂ from Oxidating DC-Sputtered Metallic Tin (Sn) for Efficient and Stable Perovskite Solar CellsACS Applied Materials & Interfaces · 2025
- Scalable Deposition of YCl 3 ‐Passivated High‐Quality SnO 2 Electron Transport Layer for Perovskite Solar ModulesAdvanced Functional Materials · 2026
- Tin oxide thin films for the future: A paradigm shift in property engineering for advanced functional devicesNext Materials · 2025
- Surface Fluorination of ALD Tin Oxide by SF 6 Plasma for Operationally Stable Perovskite Solar CellsAdvanced Optical Materials · 2026
- Gluconic Acid Ligand Enables Rapid Chemical Bath Deposition of SnO2 for High-Efficiency Perovskite Solar Cells.Small (Weinheim an der Bergstrasse, Germany) · 2026