From the paper's conclusion- This article highlights the value of trace diboron for forming desirable electrolyte interphases to obtain the wonderful long-term cycle performance and rate performance of Li||NCM811 cells.
Abstract
Developing efficient, low-cost, multifunctional additives that require small amounts and can simultaneously protect both the cathode and anode remains a major challenge for the practical application of lithium batteries. Herein, bis(2,4-dimethylpentane-2,4-glycolato)diboron (B2hmp2) was introduced to construct a greatly Li+-conductive cathode electrolyte interphases (CEIs) at the LiNi0.8Co0.1Mn0.1O2 (NCM811) surface together with robust solid electrolyte interphases (SEIs). Using a common electrolyte with 0.2 wt % B2hmp2, the Li||Li cells deliver markedly enhanced long-cycling stability, sustaining stable operation for 500 h at 0.5 mA cm-2. Furthermore, following 350 cycles at 0.5 C, the capacity retention of 4.5 V Li||NCM811 cells was elevated from 57.2 to 83.6%. Experimental results reveal that the thin, uniform, boron-rich CEI generated by B2hmp2 effectively mitigates particle microcracking and restrains the dissolution of transition metal ions. Interface analysis reveals that the modified SEI film enriched with B-O species and LiF facilitates uniform Li plating/stripping without dendrite formation and reduces the continuous parasitic decomposition of electrolyte solvents. This article highlights the value of trace diboron for forming desirable electrolyte interphases to obtain the wonderful long-term cycle performance and rate performance of Li||NCM811 cells.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Electrolyte Sustaining 4.5 V Li||NCM811 Batteries Cycled at 80°CAdvanced Energy Materials · 2026
- Steric and Electronic Synergy of CEI Modifier Regulates Bulk and Interphase for 4.5 V Li||NCM811 Batteries.Nano letters · 2026
- Complementary Functional-Group Integration Directs Interphase Chemistry toward High-Temperature Stable Ni-Rich CathodesACS Sustainable Chemistry & Engineering · 2026
- Ultra‐Stable High‐Voltage Cycling of Li‐Ion Batteries via Interphase Engineering with 3,5‐Bis(trifluoromethyl)phenyl IsocyanateAdvanced Functional Materials · 2026
- Multifunctional Electrolyte Additive toward Moisture‐Tolerant, High Voltage (4.8 V) and Wide Temperature (−10 to 60 °C) Adaptable Lithium‐Ion BatteryAdvanced Energy Materials · 2025
- Nitrobenzo Crown Ether Enables Stable Interphases in Lithium Metal BatteriesAdvanced Functional Materials · 2026