Interstitial Cu-Induced Band Structure and Phonon Transport Regulation for Eco-friendly n-Type SnSe2 Thermoelectric Power Generation.

Wenxin Lai, Pengfei Xu, Molly Meng-Jung Li, Biao Xu

School of Chemistry and Chemical Engineering, Nanjing University of Science and Technology, Nanjing210094, China. · State Key Laboratory of Flexible Electronics (LoFE) & Institute of Advanced Materials (IAM), School of Materials Science and Engineering, Nanjing University of Posts & Telecommunications, Nanjing210023, China.

Key points

From the paper's conclusion
  • Develop a CuCl annealing strategy to leverage Cu interstitial intercalation for the precise modulation of electronic band structures and phonon dispersions in SnSe2, synergizing with the Cu-induced formation of SnSe heterojunctions to effectively decouple electron and phonon transport.
  • The SnSe2-2 mol% CuCl sample achieves a maximum power factor (PF) of 0.74 mW m-1 K-2 and surpasses pristine SnSe2 by 8-fold, with a κL reduced to 0.53 W m-1 K-1 at 723 K, marking a 31% decrease relative to pristine SnSe2, and a dimensionless figure of merit (zT) of 0.88 at 723 K.
  • A sustainable and high-performance paradigm for green energy harvesting is unlocked by effectively decoupling electronic and thermal transport in eco-friendly SnSe2.

Abstract

Layered n-type SnSe2 is a promising eco-friendly thermoelectric (TE) material, yet its practical application is constrained by low carrier concentration and the inherent coupling of electronic-thermal transport. Herein, a CuCl annealing strategy is developed to leverage Cu interstitial intercalation for the precise modulation of electronic band structures and phonon dispersions in SnSe2. By synergizing with the Cu-induced formation of SnSe heterojunctions, this approach effectively decouples electron and phonon transport. Consequently, the SnSe2-2 mol% CuCl sample achieves a maximum power factor (PF) of 0.74 mW m-1 K-2 and surpasses pristine SnSe2 by 8-fold. Furthermore, the κL is reduced to 0.53 W m-1 K-1 at 723 K, marking a 31% decrease relative to pristine SnSe2. This translates to a dimensionless figure of merit (zT) of 0.88 at 723 K parallel to the spark plasma sintering direction. Notably, we fabricate the first SnSe2-based single-leg thermoelectric generator (TEG), which delivers an energy conversion efficiency of about 2% under a ΔT of 340.8 K. By effectively decoupling electronic and thermal transport, this work unlocks the full potential of eco-friendly SnSe2, providing a sustainable and high-performance paradigm for green energy harvesting without relying on toxic elements.

Read the paper

Discussion · 1

Science Skim's AI key points, plus readers' public thoughts

Science SkimAI key points
Pinned
  • Develop a CuCl annealing strategy to leverage Cu interstitial intercalation for the precise modulation of electronic band structures and phonon dispersions in SnSe2, synergizing with the Cu-induced formation of SnSe heterojunctions to effectively decouple electron and phonon transport.
  • The SnSe2-2 mol% CuCl sample achieves a maximum power factor (PF) of 0.74 mW m-1 K-2 and surpasses pristine SnSe2 by 8-fold, with a κL reduced to 0.53 W m-1 K-1 at 723 K, marking a 31% decrease relative to pristine SnSe2, and a dimensionless figure of merit (zT) of 0.88 at 723 K.
  • A sustainable and high-performance paradigm for green energy harvesting is unlocked by effectively decoupling electronic and thermal transport in eco-friendly SnSe2.