ACS applied materials & interfaces

A Self-Catalyzed, Seed-Regulated Nucleation-Growth Strategy for Ambient-Pressure-Dried Transparent Aerogels Combining Mechanical Robustness and Thermal Insulation.

Mengguo Li, Meixue Liu, Ziping Zhou, Jianjun Shi, Qifang Li, Guangxin Chen, Zheng Zhou

Key Laboratory of Carbon Fiber and Functional Polymers, Ministry of Education, College of Material Science and Engineering, Beijing University of Chemical Technology, Beijing100029, China. · Aerospace Research Institute of Materials and Processing Technology, Science and Technology on Advanced Functional Composites Technology , Beijing100076, China.

Key points

From the paper's conclusion
  • The resulting aerogel exhibited a visible-light transmittance of up to 88.86%, a low thermal conductivity of 23.1 mW·m–1·K–1, a maximum deformation of 63.7% with a compressive strength of 12.12 MPa, and an initial decomposition temperature (Td5) of 520 °C.

Abstract

Although transparent insulating aerogels are promising for energy-efficient glazing, their practical application remains limited by optical scattering, structural inhomogeneity, poor mechanical properties, and complex preparation processes. Herein, we report an octa(tetramethylammonium) polyhedral oligomeric silsesquioxane (OctaTMA-POSS)-regulated nucleation-growth strategy to fabricate mechanically robust transparent aerogels via ambient-pressure drying. Methyltriethoxysilane (MTES) was used as the precursor, and OctaTMA-POSS served as a multifunctional nanobuilding block whose intrinsic alkaline catalytic activity eliminated the need for additional acid or base catalysts. The rigid POSS cage acted as a seed-like nucleation center and was incorporated into the aerogel skeleton to regulate primary-particle growth and reinforce the framework. In situ monitoring of the gelation process revealed that this strategy effectively regulated primary-particle growth, yielding a fine, uniform nanoporous skeleton. The resulting aerogel exhibited a visible-light transmittance of up to 88.86%, a low thermal conductivity of 23.1 mW·m-1·K-1, a maximum deformation of 63.7% with a compressive strength of 12.12 MPa, and an initial decomposition temperature (Td5) of 520 °C. This work provides a simple and cost-effective route to high-performance transparent insulating aerogels for energy-efficient glazing and building-envelope applications.