Nanoscale Mechanisms of Corrosion Threshold: Effects of Passivation Film Crystal Structures.
Muhan Wang, Yihan Wang, Ziye Li, Pan Wang, Xiangming Zhou, Jinrui Zhang, Shuxian Hong, Dongshuai Hou
Department of Civil Engineering, Qingdao University of Technology, Qingdao266033, China. · Department of Engineering, Brunel University London, Uxbridge, MiddlesexUB8 3PH, United Kingdom.
Key points
From the paper's conclusion- The results indicate that polymorph-dependent coordination stability and interfacial depassivation energetics contribute to the macroscopic corrosion threshold, although they do not fully account for the complexity of corrosion initiation in real systems.
Abstract
The corrosion resistance of passive films on reinforcing steel is fundamentally governed by the depassivation stability of iron oxide polymorphs under chloride-containing environments. In this study, the electrochemical behavior and atomistic depassivation mechanisms of γ-, β-, and α-Fe2O3 passive films were systematically investigated through combined electrochemical measurements, structural characterization, metadyn2amics, and reactive force field (ReaxFF) molecular dynamics simulations. Electrochemical results demonstrate that β-Fe2O3 exhibits the lowest corrosion current density, the highest impedance stability, and the strongest resistance against chloride-induced depassivation. Across 0-5 wt % NaCl, the β-Fe2O3-dominant coating exhibited the lowest mean corrosion-current response and a comparatively persistent impedance response. At 5 wt % NaCl, the corrosion current density was (5.46 ± 0.65) × 10-5 A for the β-dominant coating, compared with (7.11 ± 0.19) × 10-5 A for the γ-dominant in situ film and (3.45 ± 1.24) × 10-4 A for the α coating (mean ± SD, n = 3). Metadynamics simulations reveal that β-Fe2O3 maintains the highest free-energy barrier for Fe atom exfoliation even at elevated NaCl concentrations, indicating intrinsically superior thermodynamic stability. At 5 wt % NaCl, the calculated Fe-exfoliation barriers were approximately 55, 21, and 10 kJ mol-1 for the β-, γ-, and α-Fe2O3 models, respectively. Atomic-scale analyses further show that the β-phase suppresses chloride penetration, limits interfacial hydration accessibility, and preserves stable Fe-Os coordination networks. In contrast, γ- and α-Fe2O3 undergo significant hydration-assisted coordination exchange and lattice destabilization under chloride exposure. The results establish that the macroscopic corrosion threshold is partly associated with polymorph-dependent coordination stability and interfacial depassivation energetics. The results indicate that polymorph-dependent coordination stability and interfacial depassivation energetics contribute to the macroscopic corrosion threshold, although they do not fully account for the complexity of corrosion initiation in real systems.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Passive film evolution on Ni-Cr-Mo alloys in acidic chloride solution during anodic polarizationCorrosion Communications · 2025
- Multiscale Characterization of Phase-Specific Oxide Evolution: Linking Microstructure and Electrochemical Response During H2O2-Induced β-Phase Dissolution of Ti–6Al–4VMaterials · 2026
- Mechanistic insights into pitting potential, incubation time and critical temperature: An extension of the Point Defect ModelCorrosion Communications · 2026
- Unveiling Phase-Dependent Fe-O Bond-Guided Nitrate Reduction at Biocathodes: Balancing Interfacial Reactivity and Iron Bioavailability.Environmental science & technology · 2026
- Effect of Ni Content on the Microstructure, Corrosion Resistance, and High‐Temperature Oxidation of Fe–Cr–Si Alloyssteel research international · 2026
- Ultrathin SrTiO3 Capping Stabilizes the Surface Chemistry of Brownmillerite Ferrites during ReductionNano Letters · 2026