ACS applied materials & interfaces

Polymer Coating Adhesion Drives Functional and Biological Outcomes in Meniscus Implants.

Alfonso F Blanco, Inés Rubio-Prego, Carmen Bao-Varela, Rebeca Bouza, Paulina Nuñez Bernal, Riccardo Levato, Jos Malda, Elizaveta Kon,

University of Santiago de Compostela, Center for Research in Molecular Medicine and Chronic Diseases (CiMUS), Health Research Institute of Santiago de Compostela (IDIS), Santiago de Compostela15706, Spain. · University of Santiago de Compostela, Photonics4Life Group, Faculty of Physics and Faculty of Optics and Optometry, Materials Institute (iMATUS), Santiago de Compostela15782, Spain.

Key points

From the paper's conclusion
  • These findings support the use of an ECA interlayer to integrate a bilayer drug-releasing coating with a PCU meniscus implant while preserving construct-level mechanical behavior and drug release under the conditions evaluated.

Abstract

Achieving stable integration of drug-releasing polymer coatings with load-bearing meniscus implants remains a challenge in biomaterials engineering. In this study, four surface modification strategies, femtosecond-pulsed laser treatment, oxygen plasma, polydopamine, and an ethyl-2-cyanoacrylate (ECA) interlayer, were evaluated for the integration of a dexamethasone (DEX)- and celecoxib (CLX)-releasing bilayer coating with a polycarbonate urethane (PCU) meniscus implant. The selected construct comprised an ECA interlayer applied from a 40% (w/v) solution, a CLX-loaded PLLA/PCL layer prepared at 100 mg/mL and a 53/47 (w/w) polymer ratio with 16.6% CLX loading, and an outer DEX-loaded PLGA layer prepared at 200 mg/mL with 2.44% DEX loading. At 37 °C, compared with uncoated PCU, ECA-containing constructs showed significantly higher storage modulus, loss modulus, and elastic modulus (p < 0.05), while tan δ remained unchanged, indicating preservation of the elastic-dominant viscoelastic response of the complete construct. The ECA-containing coating was subsequently adapted to the geometry of a sheep meniscus implant using an optimized dip-coating procedure. During a 21-day bioreactor study, repeated compression and shear increased cumulative DEX release from 59 to 67% and CLX release from 25 to 40% relative to static controls, while no visible coating delamination was observed. Ethylene oxide sterilization preserved drug loading and release behavior. In an exploratory three-month sheep study, the fiber-fixed coated implants remained in position, and the coating remained macroscopically associated with the retrieved prostheses. These findings support the use of an ECA interlayer to integrate a bilayer drug-releasing coating with a PCU meniscus implant while preserving construct-level mechanical behavior and drug release under the conditions evaluated.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers