Heparin-Ornamented Polycaprolactone-Silk Fibroin Emulsion-Based Nano-/Microfibrous Conduit as a Promising Hemocompatible Tubular Graft.
Trina Roy, Preetam Guha Ray, Bency Shaji, Ragavi Rajasekaran, Debajyoti Palai, Abhijit Lincon, Pravin Vasudeo Vaidya, Nantu Dogra,
School of Medical Science and Technology, Indian Institute of Technology Kharagpur, Kharagpur, West Bengal721302, India. · Department of Metallurgical and Materials Engineering, Indian Institute of Technology Kharagpur, Kharagpur, West Bengal721302, India.
Key points
From the paper's conclusion- This study explored the grafting of heparin on the polycaprolactone (PCL)-silk fibroin (SF) composite fabricated as emulsion electrospun core-shell fibers, followed by O2 plasma modification and silanization with 3-(aminopropyl) triethoxysilane (APTES).
Abstract
The essential prerequisite of a vascular conduit is to provide a conducive, healthy lumen interface to the flowing blood within it. The persistent problem of late thrombosis, coagulation cascade activation, and vessel occlusion is pertinent in commercial and small-diameter vascular grafts (SDVG) (<6 mm diameter), upon coming in contact with blood flow. The above critical issues are overcome by providing an anticoagulant and antithrombotic coating to the lumen surface. This study explored the grafting of heparin on the polycaprolactone (PCL)-silk fibroin (SF) composite fabricated as emulsion electrospun core-shell fibers, followed by O2 plasma modification and silanization with 3-(aminopropyl) triethoxysilane (APTES). The density of heparin on PSH5 surfaces was ∼18.43 µg/cm2, sufficiently higher than in previous studies. Heparin-grafted fibers (PSH3 and PSH5) exhibited exceptional hemocompatibility with hemolysis % of (∼0.2 ± 0.003), maintaining a platelet discoid shape (∼3.5-3.9 µm diameter) without platelet activation/aggregation and conserving disc-shaped RBC morphology without apoptosis (∼5.6-5.8 µm diameter). PSH5 fibers further supported human umbilical vein endothelial cell (HUVEC) growth and proliferation on their surfaces with % cell viability of 121.8% after 5 days, with observation of the CD31 + HUVEC confluent monolayer in in vitro studies for 12 days. Subcutaneous in vivo implantation of PSH5 also depicted sufficient muscular layers and collagen deposition after 60 days of implantation with neovasculatures.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Heparin-Immobilized Polyurethane with Biomimetic Structure and Enhanced Hemocompatibility for Small-Diameter Vascular GraftsPolymers · 2026
- Heparin-grafted aligned chitosan/silk fibroin scaffolds with multifunctional bioactivities for cardiovascular applications.Colloids and surfaces. B, Biointerfaces · 2026
- Heparin and adipose stem cell exosome functionalization improves performance of SIS/PLCL small-diameter vascular grafts.Journal of advanced research · 2026
- Electrospun Heparin-Loaded PCL Nanofiber Sutures with Sustained Release for Antithrombotic Applications.Pharmaceuticals (Basel, Switzerland) · 2026
- Tunable Bioresorbable Scaffolds With Marine Sulfated Polysaccharides for Small‐Caliber Vascular Grafts: A Multi‐Layered Strategy Combining Electrospinning and 4‐Axis PrintingAdvanced Healthcare Materials · 2026
- Heparin- and Selenocystamine-Functionalized Silk Fibroin Hydrogel for Anticoagulation and Catalytic Nitric Oxide GenerationACS Omega · 2026