Exposure-Consistent Hydrogen Boundary Conditions Derived from Reactive Molecular Dynamics of Methane Decomposition on Nickel Surfaces
Emmanuel Peters-Teke Tebo, Sina Karimzadeh, Tien-Chien Jen
Key points
From the paper's conclusion- These results show that the surface with the largest normalized Ni-associated H inventory does not necessarily have the largest geometric subsurface fraction.
Abstract
Hydrogen-assisted degradation of metals is governed by the local hydrogen population available at near-surface lattice sites and defects. However, atomistic mechanical simulations commonly employ hydrogen concentrations that are not representative of realistic exposure conditions. In this study, ReaxFF-based reactive molecular dynamics is used to translate sustained CH4 and CH4 + H2O exposure on a Ni(211) surface under an accelerated closed-cell protocol at 1000–1350 K into exposure-conditioned hydrogen availability descriptors. Three independent trajectories are performed for each exposure-temperature condition to quantify the normalized Ni-associated H inventory, hydrogen partitioning between adsorbed and subsurface regions, and localization across CN-defined step and terrace regions. A key finding is a dry–wet inversion in hydrogen accessibility. Although CH4 + H2O exposure produces a larger normalized Ni-associated H inventory (θH = 0.67–0.77), 71.6–86.1% of that inventory is primarily O-bound, while less than 3.5% of the geometrically defined near-surface H population lies within the subsurface window. In contrast, CH4-only exposure yields a smaller normalized Ni-associated H inventory (θH = 0.088–0.447) but substantially greater subsurface partitioning, reaching 12.3% at 1350 K. These results show that the surface with the largest normalized Ni-associated H inventory does not necessarily have the largest geometric subsurface fraction. Furthermore, CH4 + H2O suppresses carbon accumulation, sustains an oxygen-containing surface state, and maintains higher per-site hydrogen localization around CN-defined step regions. Additional Ni(111) and laterally doubled Ni(211) checks retain the wet-over-dry H areal-density ordering and the complementary dry-over-wet subsurface-fraction ordering at 1250 K. The resulting protocol-specific descriptors provide candidate inputs for controlled downstream simulations of hydrogen transport, trapping, and degradation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Origins of the hydrogen spillover effect in d-block metalsNature Communications · 2026
- Quenching or Accelerating Large-Scale Surface Reconstruction by the Lightest Element: Facet-Dependent Hydrogen-Induced Reconstruction (HIR).Angewandte Chemie (International ed. in English) · 2026
- Bridging the Pressure Gap in Hydrogenation of CO₂ to Formate on Cu(100) by Machine Learning Molecular Dynamics and First-Principles Microkinetic ModelingACS Catalysis · 2026
- Hydride-induced palladium self-diffusion and surface restructuring on Pd(111).Nature communications · 2026
- Liquid-Metal-Induced Metal-Support Interactions for CO2 Hydrogenation.Journal of the American Chemical Society · 2026
- Formation of Dynamic Nanoporous Shells on Bimetallic Particles During Carbon Dioxide HydrogenationACS Nano · 2026