Structure Rebuilding Time-Dependent Behavior of NaMnt Gels in Aging and Stepdown Shear Stress Response: Hectorite Comparison and the Layer Charge Hypothesis.
Yee-Kwong Leong, Peta L Clode
Department of Chemical Engineering, The University of Western Australia, 35 Stirling Highway, Crawley, WA6009, Australia. · Centre for Microscopy, Characterization and Analysis, The University of Western Australia, 35 Stirling Highway, Crawley, WA6009, Australia.
Key points
From the paper's conclusion- It also made the time-dependent behavior in the stepdown shear stress response milder and caused it to disappear at 0.1 M KCl for NaMnt and 0.01 M KCl for hectorite.
Abstract
The NaMnt (SWy-2) gels displayed structure rebuilding (SB) time-dependent behavior in the stepdown shear stress response at pH from 3 to 11. The electric double layer (EDL) face-face repulsion remained strong even at pH 3, to slow the edge-face bonding in forming the network. The strong EDL repulsion at pH 3 is solely due to its high permanent layer charge density of -0.11 C·m-2. Hectorite gel commenced to show time-independent SB behavior at pH ∼ 8. Its silica face charge density was at least as high as -0.11 C·m-2 at pH 8 with the layer charge contributing -0.08 C·m-2. The negative silica face charge density was postulated to be moderated by the relatively high positive edge charges of the lath-like hectorite platelet because of its high edge-to-face area ratio of 0.24 compared to only 0.0081 for NaMnt. Salt increased the structure rebuilding speed by creating more low-energy paths to edge-face bonding. It increased the bond density and strength reflected by the larger yield stress and shear stress. It also made the time-dependent behavior in the stepdown shear stress response milder and caused it to disappear at 0.1 M KCl for NaMnt and 0.01 M KCl for hectorite. Increasing the platelet charge density by adsorbed P2O74- made the 0.1 M KCl NaMnt gel display the time-dependent behavior. In aging where an imposed shear is absent, the 0.1 M KCl NaMnt gel continued to display time-dependent structure rebuilding behavior. The faster structure rebuilding speed at higher salt concentrations is also reflected by the smaller time constant of the Leong model used to fit the aging data. The pH-dependent charge contribution to NaMnt face charge density at pH 8 is small, ∼27%. NaMnt gel behavior is more stable and less sensitive to pH change.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Salt-Controlled Hyperaging, Viscosity Bifurcation, and Stress Buildup in Aqueous Clay DispersionsIndustrial & Engineering Chemistry Research · 2026
- Rheological characterisation of clay-cement sealing suspensions with fractionated coal fly ashesScientific Reports · 2026
- Salt-Induced Nanoparticle Aggregation Decouples Mechanical Reinforcement and Ionic Transport in Polymer Nanocomposite Electrolytes.ACS macro letters · 2026
- A colloidal interaction energy barrier approach to make spherical ZrO2 suspensions time-dependent in ageing - the slow bonding effect.Physical chemistry chemical physics : PCCP · 2026
- Cyclic Nanoindentation of Clay Minerals: Micromechanical Insights Into Caprock Integrity for Subsurface Energy StorageRock Mechanics and Rock Engineering · 2026
- Structural and crystal-chemical response of glauconite globules to pH under static aqueous conditionsClays and Clay Minerals · 2026