Interface Analysis of Al2O3 on Chemically Cleaned and Plasma-Treated Germanium and Si1– x Ge x Caps in Compressively Strained Germanium on Silicon

Shahin Honari, Parinaz Tabrizian, Weihong Jiang, Yousef Karimi Yonjali, Sergei Studenikin, Maksym Myronov, Khaled Mnaymneh

Key points

From the paper's conclusion
  • Here we investigate the surface oxidation of germanium and Si1–xGex after the deposition of Al2O3.

Abstract

Here we investigate the surface oxidation of germanium and Si1–xGex after the deposition of Al2O3. The surface is analyzed using transmission electron microscopy (TEM) and X-ray photoelectron spectroscopy (XPS) techniques to see the oxidation states and to calculate the concentration of oxides at the interface. It is highly likely that the oxide at the interface forms during the deposition, with silicon showing more oxidation than germanium. Different precleaning processes were performed on the sample to compare the effect on interface oxides. Hydrogen plasma pretreatment was also used to reduce oxidation at the interface during deposition. Hydrogen plasma also changes the oxidation states of both germanium and silicon to higher oxidation states.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers