From the paper's conclusion- To address the requirements of high-strength and lightweight performance in an aluminum alloy foam board, this study proposes a multiscale interfacial strengthening strategy combining the porous architecture of aluminum foam with in situ grown ceria-zirconia hybrid nanowires to improve the tensile shear strength of 30 wt % carbon fiber-reinforced polyphenylene sulfide-aluminum foam (30 wt % CF/PPS
Abstract
To address the requirements of high-strength and lightweight performance in an aluminum alloy foam board, this study proposes a multiscale interfacial strengthening strategy combining the porous architecture of aluminum foam with in situ grown ceria-zirconia hybrid nanowires to improve the tensile shear strength of 30 wt % carbon fiber-reinforced polyphenylene sulfide-aluminum foam (30 wt % CF/PPS-aluminum foam) joints fabricated through injection molding. Metal oxide nanowires were in situ grown on the aluminum foam surfaces through a hydrothermal reaction followed by high-temperature calcination. The characterization and simulations analysis testify that the metal oxide nanowires grown on the aluminum foam surfaces and within the pores provide abundant chemically active sites and facilitate the infiltration of the PPS melt. The combined effects of the microscale pore structure and the nanowires create a multiscale mechanically interlocked interface. The active sites enable coordination interactions on the metal side and meanwhile provide local chemisorption and hydrogen-bonding interactions on the polymer side. Benefiting from the synergistic strengthening of multiscale mechanical interlocking and chemical bonding, the joints achieve a maximum tensile shear strength of 36.2 MPa.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Enhanced Mechanical Performance of SiCNWs@C/SiC Composites With a C Interphase via In Situ Polymerization‐CarbonizationInternational Journal of Applied Ceramic Technology · 2026
- Microstructure and Mechanical Properties of Solid-State Sintered SiC Brazed with a Novel Si-Ti-Al/Mo Composite FillerCoatings · 2026
- Enhancing the Comprehensive Properties of Polypropylene Films via Organic–Inorganic Interfacial Molecular EngineeringPolymer Engineering & Science · 2026
- Direct joining of Cu–Zn alloy/polymer hybrid composites via synergistic mechanical interlocking and triazine-mediated molecular interfacial bondingAdvanced Composites and Hybrid Materials · 2026
- Interface Strengthening of Brittle AgNW-MXene Composite Films through PVA or WPU Polymers for Flexible Electromagnetic Interference Shielding Applications.Langmuir : the ACS journal of surfaces and colloids · 2026
- Laser-assisted fabrication of AISI 1018 steel–PET–steel sandwich composites with surface-engineered interfaces: Mechanical and chemical insightsJournal of Adhesion Science and Technology · 2026