Structural Evolution and Polymorph-Dependent Thermoelectric Properties of In2Se3

Xi Peng, Xili Wen, Lin Liao, Han Xu, Xiyun Zhang, Lingxiao Yu, Ying Huang, Tingting Luo,

Key points

From the paper's conclusion
  • These results connect thermal-history-dependent polymorph selection with electronic and phonon transport in bulk In2Se3.

Abstract

Van der Waals semiconductor In2Se3 exhibits multiple polymorphs, yet the thermal-history-dependent selection of bulk polymorphs and its relationship with transport remain unclear. Here, phase-pure bulk α(2H)-, α(3R)-, and γ-In2Se3 are obtained by controlling quenching temperature, cooling conditions, and annealing duration. Ex situ annealing of bulk ingots reveals staged retained-phase evolution from α(2H) through a transient α(3R)-enriched state to γ-In2Se3, consistent with Ostwald’s rule of stages. At 673 K, the estimated α(3R) fraction in the initially α(2H) sample reaches approximately 74–78% after 2–3 h and subsequently decreases as γ-In2Se3 develops. For the two α polymorphs, the room-temperature electrical conductivity along the ∥ specimen direction increases from 2 S m–1 for α(2H)-In2Se3 to 86 S m–1 for α(3R)-In2Se3. Despite its lower carrier concentration, α(3R)-In2Se3 exhibits a substantially higher estimated mobility of 20.9 cm2 V–1 s–1, compared with 0.20 cm2 V–1 s–1 for α(2H)-In2Se3. The thermal conductivity along the same direction decreases from 3.19 to 2.70 W m–1 K–1, consistent with the lower measured sound velocities and lower calculated low-frequency phonon group velocities of α(3R)-In2Se3. These results connect thermal-history-dependent polymorph selection with electronic and phonon transport in bulk In2Se3.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers