Key points
From the paper's conclusion- Overall, the ability of BDDPA to inhibit sorbent degradation under dry and humid, CO 2 -free and CO 2 -containing (0.04%) air at intermediate (70 °C) and elevated (120 °C) temperatures is promising in prolonging sorbent stability and underscores the importance of performing accelerated oxidation studies in the presence of all species that are expected to be present in DAC processes to identify sui
Abstract
High Resolution Image Download MS PowerPoint Slide Solid amine sorbents have shown promise in the removal of ultradilute CO 2 from the atmosphere. Despite being a promising candidate material type for this application, these sorbents are prone to degradation during long-term exposure to environmental components such as CO 2, O 2, and H 2 O, with amine oxidation being a particularly challenging problem. In this study, we investigate the potency of different radical scavengers and additives in mitigating the degradation of a model poly(ethylenimine) (PEI)/Al 2 O 3 sorbent under direct air capture (DAC)-relevant conditions. The results reveal that a 4,4′-bis(α,α-dimethylbenzyl)diphenylamine (BDDPA)-incorporated PEI/Al 2 O 3 sorbent showed the most resistance toward oxidative degradation at varying exposure times and BDDPA loadings under CO 2 -free air (21% O 2 /balance N 2 ) at 120 °C. Interestingly, under humid (∼43% relative humidity (RH) at 26 °C) and dry 0.04% CO 2 -air, the BDDPA/PEI/Al 2 O 3 sorbent showed enhanced sorbent stability both at 70 and 120 °C after 4.5 h of exposure. Under humid CO 2 -free air, at 120 °C, the antioxidant performance slightly declined (in comparison to the dry CO 2 -free air condition) but displayed a much higher stability than the pristine sorbent. Overall, the ability of BDDPA to inhibit sorbent degradation under dry and humid, CO 2 -free and CO 2 -containing (0.04%) air at intermediate (70 °C) and elevated (120 °C) temperatures is promising in prolonging sorbent stability and underscores the importance of performing accelerated oxidation studies in the presence of all species that are expected to be present in DAC processes to identify suitable stabilization treatments for sorbent materials.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of Transition Metal Ion Contaminants on the Performance of Amine-Based Solid Sorbents in Direct Air CaptureEnvironmental Science & Technology · 2026
- Epoxide-Modified Diethylenetriamine for Ambient-Temperature Direct Air CaptureACS Applied Materials & Interfaces · 2026
- Predicting Oxidative Degradation of Aminopolymer Adsorbents for CO2 Direct Air Capture via Time−Temperature Superposition of Accelerated Aging DataACS Engineering Au · 2026
- Toward Stable CO₂ Capture in Combined Cycle Gas Turbine Flue Gas: Degradation-Resistant Biphasic Absorbents Enabled by Amine Blending and Radical ScavengingEnergy & Fuels · 2026
- Direct Air Capture of CO2 with Amine-Functionalized Solid Sorbents: Material Performance, Contactor Design, and Engineering Scale-UpProcesses · 2026
- In situ azetidine polymerization elevates the performance of commercial polymer resin sorbents in carbon dioxide capture.Science advances · 2026