Lithium Makes the DifferenceEvolution of Lithium Vacancy Disorder during Temperature-Induced Phase Transitions of the Li-Ion Conductor Li4SnS4.
Lucas G Balzat, Sebastian Bette, Jakob Blahusch, Christian Schneider, Emmanuelle Suard, Anjali Menakath, Kristina Gjorgjevikj, Simon Krause,
Max Planck Institute for Solid State Research, Department of Nanochemistry, Heisenbergstraße 1, Stuttgart 70569, Germany. · Institut Laue-Langevin, 71 avenue des Martyrs CS 20156, Grenoble 38042, Cedex 9, France.
Key points
From the paper's conclusion- Two orthorhombic Li4SnS4 polymorphs (α and β) are known, and their temperature-dependent phase behavior was explored
- α-Li4SnS4 transitions to β-Li4SnS4 at 96 °C, and a second, previously unknown reversible phase transition from β-Li4SnS4 to a new γ-polymorph at 196 °C was identified
- Li4SnS4 transitions from the lithium-vacancy-disordered α-phase to the ordered β-phase and finally to the disordered γ-Li4SnS4
Abstract
Sulfide-based lithium-ion solid electrolytes are promising candidates for solid-state batteries due to their high ionic conductivities, although they typically exhibit high moisture sensitivity. Li4SnS4 has recently attracted scientific interest because it exhibits higher moisture resistance than most other sulfide electrolytes. Two orthorhombic Li4SnS4 polymorphs (α and β) are known, yet their temperature-dependent phase behavior remains unexplored. Differential scanning calorimetry and temperature-dependent powder X-ray diffraction revealed that α-Li4SnS4 transitions to β-Li4SnS4 at 96 °C. Furthermore, we identified a second, previously unknown reversible phase transition from β-Li4SnS4 to a new γ-polymorph at 196 °C. Other phase transitions from -150°C to 1000°C were not identified. All polymorphs crystallize in space group Pnma (no. 62) and feature identical zig-zag-like arrangements of SnS4 4- tetrahedra. The main structural differences lie in the ordering of the lithium substructure. By combining temperature-dependent powder X-ray and neutron diffraction with high-temperature 7Li and 119Sn NMR as well as Raman spectroscopy, we show that Li4SnS4 transitions from the lithium-vacancy-disordered α-phase to the ordered β-phase and finally to the disordered γ-Li4SnS4. Using electrochemical impedance spectroscopy, we measured ionic conductivities from 10-6 S cm-1 to 10-1 S cm-1 between 25 °C to 220 °C. Conductivity changes are gradual, consistent with the subtle structural variations among all polymorphs.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- Two orthorhombic Li4SnS4 polymorphs (α and β) are known, and their temperature-dependent phase behavior was explored
- α-Li4SnS4 transitions to β-Li4SnS4 at 96 °C, and a second, previously unknown reversible phase transition from β-Li4SnS4 to a new γ-polymorph at 196 °C was identified
- Li4SnS4 transitions from the lithium-vacancy-disordered α-phase to the ordered β-phase and finally to the disordered γ-Li4SnS4
Readers' thoughts
No reader thoughts yet.
Related papers
- Kinetic Control of Polymorphism in Li10.5Si1.5P1.5S12-Based Solid Electrolytes.Journal of the American Chemical Society · 2026
- Quaternary Solid Electrolytes of the Na11Sn2PS12 Type with an Sn/Group 5-Metal CombinationInorganic Chemistry · 2026
- Can sulfide solid electrolytes for lithium-ion batteries be handled in dry rooms? – A multiprobe approachEnergy storage materials · 2025
- Conductivity activation of LISICON electrolytes via polar molten salt modulation for solid state Li batteries.Journal of colloid and interface science · 2026
- Machine Learning-Assisted Crystal Structure Prediction of Solid-State Electrolytes Reveals Superior Ionic Conductivity in Metastable Edge-Sharing PhasesJournal of the American Chemical Society · 2025
- High-Entropy Design for Improving Ionic Conductivity and Air Stability of Lithium Argyrodites for All-Solid-State Lithium-Sulfur Batteries.Small methods · 2026