From Halide Formation to Incorporation: The Role of Halogen Identity in the Solid−Electrolyte Interphase Formation
Manuel Reiter, Travis P. Pollard, Oleg Borodin, Julita Tabor, Joseph Scapin, Chulgi Nathan Hong, Maria R. Lukatskaya
Key points
From the paper's conclusion- These results demonstrate that analogous halogenated additives can follow fundamentally different reduction pathways, where halogen identity controls not only targeted inorganic products but also the route through which the SEI forms.
Abstract
Designing a stable solid−electrolyte interphase (SEI) for Li−metal batteries remains a major challenge. While LiF-rich interphases are widely regarded as beneficial, the broader role of halide chemistry in SEI formation remains poorly understood. Here, we investigate how halogen identity (F, Cl, and Br) in pyridinium additives governs interphase formation pathways in ether-based electrolytes. Although chlorinated and brominated additives undergo early electroreduction (>2.5 V vs. Li/Li+), they produce SEIs with minimal halide content (∼2.5 at.%). Spectroscopic, electrochemical, and computational analyses reveal that reduced chlorinated and brominated intermediates preferentially undergo dimerization, forming soluble redox-active species that compete with interphase formation. In parallel, the substantially higher solubility of LiCl and LiBr relative to lithium fluoride limits the SEI integration of these inorganic products. As a result, chlorinated and brominated additives produce chemically heterogeneous, continuously evolving interphases enriched with carbonaceous and salt-derived species. In contrast, the fluorinated analogue undergoes efficient defluorination without detectable dimer formation, yielding a stable LiF-rich SEI. These results demonstrate that analogous halogenated additives can follow fundamentally different reduction pathways, where halogen identity controls not only targeted inorganic products but also the route through which the SEI forms.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Probing Interfacial Electrolyte Chemistry and SEI Failure Mechanisms on Lithium-Metal Anodes via Establishing a Multichannel Analysis Paradigm.JACS Au · 2026
- Chloride-functionalized electrolyte design for safe and high-energy-density lithium metal batteries.Nanoscale horizons · 2026
- Insight into the Interfacial Evolutions between Halide and Sulfide Solid ElectrolytesACS Energy Letters · 2025
- Fluorine-free gel polymer electrolyte for lithium oxide-rich solid electrolyte interphase and stable Li metal batteriesNature Communications · 2025
- Halide Anions Regulate the Self‐Assembly of HPMC Coating on PP Separator to Synergistically Modulate Weak Solvation Structure and Anode Interface to Enhance Lithium Metal BatteryAdvanced Functional Materials · 2026
- Reviewing Li2O in solid electrolyte interphases: from intrinsic properties and interfacial chemistry to rational interphase design.Nanoscale · 2026