Crystal Growth & Design

Ultra-Low Afterglow and Fast Decay LYSO Scintillation Crystal by Co-Doping of Ni and In

Zhongjun Xue, Zhe Zhang, Chengyi Li, Peng Qiu, Shuwen Zhao, Dongzhou Ding

Key points

From the paper's conclusion
  • This, in turn, significantly optimizes the afterglow level (reducing it by about 2 orders of magnitude) and reduces the scintillation decay time of the crystal (shortening it by approximately 32%).

Abstract

Cerium-doped yttrium lutetium silicate (LYSO:Ce) scintillation crystals have significant application value in the field of radiation detection due to their excellent comprehensive scintillation performance. However, their strong afterglow and relatively long scintillation decay time (∼42 ns) severely limit their application in the field of high-repetition-rate ultrafast radiation detection. To address this challenge, we propose a multi-ion co-doping strategy to optimize afterglow and decay time of LYSO:Ce crystal. A series of Ni2+, In3+ co-doped LYSO:Ce,Ni,xIn crystals were prepared using the Czochralski (Cz) method, and the regulation mechanism of Ni2+ and In3+ co-doping on the scintillation performance of the crystal was systematically investigated. It was found that the co-doping of Ni2+ and In3+ can optimally shorten the excited-state lifetime of the luminescent center Ce in the crystal by approximately 40%, significantly suppressing the deep and shallow energy level traps in the crystal. This, in turn, significantly optimizes the afterglow level (reducing it by about 2 orders of magnitude) and reduces the scintillation decay time of the crystal (shortening it by approximately 32%). The collaborative co-doping strategy proposed in this work is expected to be extended to other scintillation materials with Ce as the luminescent center, enabling efficient regulation of afterglow and scintillation decay time.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers