Janus-coated cation exchange membrane enhances anti-scaling performance in electrodialysis through divalent-ion restriction and interfacial hydration.
Yuyang Yao, Yueyue Lu, Yitao Chen, Shiyu Zhou, Jin Guo, Ruifen Tian, Yuqing Lin, Jiangnan Shen,
Key Laboratory of Materials Physics, Anhui Key Laboratory of Nanomaterials and Nanotechnology, Institute of Solid State Physics, Hefei Institutes of Physical Science, Chinese Academy of Sciences, Hefei, 230031, PR China. · College of Chemical Engineering, Zhejiang University of Technology, Hangzhou, 310014, China; State Key Laboratory of Advanced Separation Membrane Materials, Zhejiang University of Technology, Hangzhou, 310014, China; National Key Laboratory of Green Chemical Synthesis and Transformation Technology, Hangzhou, 310014, China.
Key points
From the paper's conclusion- Simulations further showed that Ca2+ and Mg2+ were mainly confined within 0 to -10 Å of the membrane surface, while deeper penetration (-30 to -45 Å) was largely suppressed.
Abstract
Inorganic scaling severely constrains the long-term electrodialysis (ED) operation in high-salinity, high-hardness wastewaters and brines, where CaCO3 and M(OH)2 (M = Ca or Mg) accelerate voltage increase and membrane resistance growth. To address this limitation, a Janus-coated cation exchange membrane (CEM) was developed to suppress scaling-induced resistance growth without altering the sulfonated polysulfone (SPSF) backbone. The asymmetric interface combined a poly(ethylenimine) (PEI)-containing layer on one side to restrict divalent-cation penetration with a highly sulfonated SPSF coating on the opposite side to promote interfacial hydration. In 10 h recirculating M(OH)2 scaling tests, the Janus PEI-SPSF-30 membrane reduced scaling-induced resistance growth by 90.0%-95.9% at current densities of 10-30 mA·cm-2 relative to pristine SPSF. Furthermore, PEI-SPSF-30 exhibited a resistance increase of only 0.68 Ω·cm2, compared with 67.97 Ω·cm2 for SPSF, corresponding to a 99.0% reduction in resistance growth after 72 h at 30 mA·cm-2. Simulations further showed that Ca2+ and Mg2+ were mainly confined within 0 to -10 Å of the membrane surface, while deeper penetration (-30 to -45 Å) was largely suppressed. This work highlights the role of interfacial asymmetry in controlling membrane scaling and provides a valuable reference for designing scaling-resistant ED membranes for resource recovery from high-salinity, high-hardness wastewaters.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Scalable Thin-Film Composite Cation Exchange Membrane for Separation of Monovalent and Divalent Cations in ElectrodialysisEnvironmental Science & Technology · 2025
- Preparation of Cross-Linked Polysulfone Anion Exchange Membrane and Its Application in Electro–Electrodialysis Purification of Wet Process Phosphoric AcidACS Omega · 2026
- Interfacially Regulated MXene‐Based Nanocomposite Membranes for Highly Selective Ion Transport and Salinity Gradient Energy HarvestingAdvanced Materials Technologies · 2026
- Inorganic Scaling in Electrodialysis: Mechanistic Insights and Impact on Energy Efficiency and Ion SelectivityEnvironmental Science & Technology · 2026
- Dense Janus membrane with designed nanostructure and surface properties for sustainable desalination from hypersaline silica wastewater in membrane distillation.Water research · 2026
- Janus Membranes for Osmotic Energy Harvesting and Flow Capacitive DeionizationChemSusChem · 2026