Waste management (New York, N.Y.)

Mechanical fragmentation of polyester textiles for controlled particle generation.

Wang Hou, Veronika Tunáková, Maroš Tunák, Jana Novotná, Dan Wang

Department of Material Engineering, Faculty of Textile Engineering, Technical University of Liberec, Studentska 1402/2, 461 17 Liberec, Czech Republic. Electronic address: wang.hou@tul.cz. · Department of Material Engineering, Faculty of Textile Engineering, Technical University of Liberec, Studentska 1402/2, 461 17 Liberec, Czech Republic.

Key points

From the paper's conclusion
  • This study varied pass number, sieve cassette configuration, and rotation speed using a 100% polyethylene terephthalate (PET) interlock fabric as a model substrate.

Abstract

Mechanical fragmentation can create engineered secondary feedstocks from waste polyester textiles, but its process-property trade-offs remain unclear. This study varied pass number, sieve cassette configuration, and rotation speed using a 100% polyethylene terephthalate (PET) interlock fabric as a model substrate. Particles were characterized by image analysis, sieving, Rosin-Rammler modeling, and SEM. Independent milling trials quantified process performance, and FTIR spectroscopy and alkaline hydrolysis evaluated chemical changes and mass-loss response. At 3000 rpm, increasing passes from C1 to C5 reduced the image-based median equivalent diameter by 35.2% with the 1.5 mm trapezoidal-perforated cassette (B1.5) and by 38.2% with the 10 mm square-perforated cassette (B10). B1.5 sieving median decreased by 59.0%, whereas rotation speeds of 1000-3000 rpm produced no consistent monotonic effect. Five-pass B1.5 and B10 trials yielded material recoveries of 84.75 ± 1.67% and 89.89 ± 1.10%, cumulative dust fractions of 7.57 ± 0.88% and 5.89 ± 0.67%, and laboratory cycle times of 82.09 ± 0.59 and 53.49 ± 0.70 min, respectively. Cutting-mill-only nominal specific electricity demands, estimated from the 5 kW nameplate power, were 11.74 ± 0.09 and 11.58 ± 0.22 kWh/kg. FTIR detected no major changes in characteristic PET bands. Under identical hydrolysis conditions, three-hour mass loss increased from 51.67 ± 2.52% for the original fabric to 78.00 ± 2.00% for A3000 × B1.5 × C5. Results establish laboratory-scale empirical relationships between cutting-mill settings and PET fragment characteristics while revealing trade-offs among size reduction, recovery, process demand, and alkaline-hydrolysis response.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Mechanical fragmentation of polyester textiles for controlled particle generation — Science Skim