Cavitation-eroded piezoelectric ceramics as finite mechano-electrochemical transducers.
Gunn Park, Jae-Woo Park
Department of Civil and Environmental Engineering, Hanyang University, Seoul 04763, South Korea. · Department of Civil and Environmental Engineering, Hanyang University, Seoul 04763, South Korea. Electronic address: jaewoopark@hanyang.ac.kr.
Key points
From the paper's conclusion- We examined four piezoelectric materials (BaTiO3, ZnO, K0.5Na0.5NbO3, and PbZr0.53Ti0.47O3) under 40 kHz ultrasonic cavitation.
Abstract
Piezoelectric ceramics are being explored as mechanically powered materials for energy-environmental processes, but the relationship between energy transduction and material durability remains unclear. We examined four piezoelectric materials (BaTiO3, ZnO, K0.5Na0.5NbO3, and PbZr0.53Ti0.47O3) under 40 kHz ultrasonic cavitation. The pressure criterion for reactive oxygen species (ROS) formation through water compression (2.8-8.1 GPa) exceeded the 1.13 GPa compressed-bubble pressure obtained from the bubble-collapse calculation. The electron-energy analysis provides a thermal-equilibrium reference rather than a prediction of plasma-derived ROS yields. The powder-free control showed only 0.7% and 1.9% tetracycline (TC) removal after 120 and 480 min, respectively. The open-circuit piezoelectric potentials calculated for 1 μm particles at the 1.13 GPa compressed-bubble pressure (9-210 V) exceeded the electrochemical thresholds (0.33-2.8 V), and the powders showed persistent contact-potential shifts up to - 318 mV and charge storage 32-55 times beyond the electrical double-layer limit. Cavitation-induced irreversible lattice strain and selective A-site ion leaching were accompanied by elbow-shaped TC degradation kinetics with performance declining from approximately 67% to 1-3% over five cycles. Mott-Schottky and impedance analyses indicated that interfacial electrochemical states were irreversibly altered. The tested powders are described here as finite mechano-electrochemical transducers whose operation is accompanied by irreversible material changes and declining activity. The relevant design criterion for sustainable piezoelectric environmental applications should include redox output, material lifetime, recoverability, and ion-release risk as well as the first-cycle activity.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Catalytic Activity of Piezoelectric and Paraelectric BaTiO3 Nanoparticles.Nanomaterials (Basel, Switzerland) · 2026
- Efficient Dynamic Piezo-Photocatalysis of Freestanding Single-Crystal BaTiO3 Membranes by Strain Gradient.Advanced materials (Deerfield Beach, Fla.) · 2026
- Electroacoustic activation of natural quartz nanoparticles for the Guareschi-Thorpe synthesis of novel pyridine derivatives.RSC advances · 2026
- A review: recent progress of piezoelectric effect coupled photocatalytic reaction: diverse mechanisms, system/structure design, characterization and applicationCatal · 2026
- Piezocatalysis: Concepts, Advances, and Opportunities.Advanced materials (Deerfield Beach, Fla.) · 2026
- Freestanding Hierarchical-Porous BCZT Thin Films Enable Efficient Ultrasonic Energy Harvesting in Soft Tissue.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026