Ultrasonics

Robot-assisted ultrasonic TOF measurement for defect-distance localization in corroded thick-walled pipelines.

Weixin Xu, Leijie Hu, Nanhui Wu, Sihan Lv, Yunfeng Tan, Dapeng Tan

College of Mechanical Engineering, Zhejiang University of Technology, Hangzhou, 310014, China; Key Laboratory of Special Purpose Equipment and Advanced Processing Technology, Ministry of Education, Zhejiang University of Technology, Hangzhou, 310023, China. · College of Mechanical Engineering, Ningbo University of Finance and Economics, Ningbo, 315175, China; Ningbo Key Laboratory of Smart Agricultural Technology and Equipment, Ningbo, 315175, China. Electronic address: tanyunfeng@nbufe.edu.cn.

Key points

From the paper's conclusion
  • Accurate defect-distance localization in corroded thick-walled pipelines remains challenging because rough inner-wall conditions destabilize probe coupling, distort ultrasonic waveforms, and reduce the reliability of time-of-flight (TOF) extraction.

Abstract

Accurate defect-distance localization in corroded thick-walled pipelines remains challenging because rough inner-wall conditions destabilize probe coupling, distort ultrasonic waveforms, and reduce the reliability of time-of-flight (TOF) extraction. This study presents a TOF-based defect-distance localization framework enabled by robot-assisted ultrasonic acquisition, integrating active pressing, surface conditioning, metered couplant delivery, and retractable probe feeding to improve measurement consistency. A variational mode decomposition (VMD)-based denoising stage is incorporated to suppress noise-dominated components while preserving the primary echo for TOF pickoff. The framework is validated on a cast-steel pipeline containing horizontal, elbow, and vertical sections, and further evaluated in a 5-m-diameter in-service hydropower pipeline. The controlled multi-position validation shows that VMD-processed measurements achieve relative localization errors below 5 %, with a mean absolute error of 2.226 mm and 94 % of the evaluated positions within 5 mm. VMD substantially improves waveform quality, while its effect on TOF repeatability is position-dependent. A traceable laser-scanning reference and uncertainty-propagation framework are established to identify the major sources of localization uncertainty. The field evaluation achieves an overall valid signal rate of 83.33 %, demonstrating the applicability of the proposed measurement workflow under realistic degraded pipeline conditions.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Robot-assisted ultrasonic TOF measurement for defect-distance localization in corroded thick-walled pipelines — Science Skim