Ultrasonics

Investigation of the microstructure and mechanical resistance of Ti2AlN/TC4 composites prepared by ultrasonic vibration-assisted laser powder directed energy deposition (LP-DED).

Bingya Li, Ping Zou, Anqi Wang, Kornel F Ehmann, Yaotian Cheng

School of Mechanical Engineering and Automation, Northeastern University, Shenyang, 110819, China. · School of Mechanical Engineering and Automation, Northeastern University, Shenyang, 110819, China. Electronic address: pzou@mail.neu.edu.cn.

Key points

From the paper's conclusion
  • This study systematically analyzes the effects of introducing Ultrasonic Vibration (UV) and varying its amplitude during the LP-DED preparation of Ti2AlN-reinforced titanium alloy composites on grain evolution, ceramic particle distribution, and the mechanical properties of the deposited layers.

Abstract

The stark thermal-property mismatch between ceramics and titanium alloys frequently triggers severe ceramic particle segregation during Laser Powder Directed Energy Deposition (LP-DED). This study systematically analyzes the effects of introducing Ultrasonic Vibration (UV) and varying its amplitude during the LP-DED preparation of Ti2AlN-reinforced titanium alloy composites on grain evolution, ceramic particle distribution, and the mechanical properties of the deposited layers. The results demonstrate that UV significantly reduces grain size, enhances the dispersion of ceramic particles, improves crystal deformation, and markedly increases the wear resistance of the composite material. In addition, as the amplitude increases, the grains first refine and then shorten, while the grain size increases accordingly. Meanwhile, as the homogeneity of the ceramic particles improves, the dislocation density increases, the intensity and uniformity of recrystallization increase, and microhardness and wear resistance improve. Compared to the without-UV sample, UV-assisted samples exhibited Average Phase Area (APA) reductions of up to 47.55%, Kernel Average Misorientation (KAM) increases of up to 25.00%, microhardness gains of up to 6.19%, and wear-depth and wear-width reductions of up to 41.40% and 20.65%, respectively. This study further investigates how the distribution of ceramic phases, grain refinement, and core-coating morphology affect load transfer efficiency and wear resistance. This establishes a foundation for the synergistic control of the microstructure and resistance of Ti2AlN/TC4 composites.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.