FTIR–XRD comparative study of pyrolysis residues obtained from plastic waste

Muslum Gurbanov, Ulviye Gulieva, Imamaddin Amiraslanov, Samir Karimov, Gunel Imanova

原始摘要(英文原文)· Original abstract
This study examines the thermal degradation of PET-1 plastic waste containers (SIRAB, Azerbaijan) using FTIR spectroscopy and XRD analysis. Samples were pyrolyzed at 350°C, 450°C, and 550°C for 1 h under inert conditions. XRD results show a progressive loss of crystallinity with increasing temperature, leading to an almost fully amorphous, carbon-rich residue at 550°C. FTIR analysis indicates significant chemical changes above ∼420°C, including the formation of carbonyl-containing compounds (∼1679 cm⁻¹) and O–H related bands (2500–3062 cm⁻¹), associated with pyrolysis products formed via chain scission.Overall, combined FTIR and XRD results confirm a temperature-dependent degradation pathway characterized by structural amorphization and the formation of oxygenated aromatic residues.
读原文 · Read the paper ↗

AI 追问PRO

登录后使用 AI 追问

讨论区

登录后参与讨论

相关论文 · Related

FTIR–XRD comparative study of pyrolysis residues obtained from plastic waste — 科研速览 Science Skim